Polymer Engineering & Science

Enhancement of Thermal and Mechanical Properties of Polyamide 612 via Incorporation of Basalt Fiber

Yi‐Cang Lai, Chao‐Kai Tseng, Chia‐Hsuan Chang, Chin‐Wen Chen

Key points

From the paper's conclusion
  • These results identify interfacial engineering and high‐loading flow behavior as priorities for further development.

Abstract

Basalt fiber (BF)‐reinforced polyamide 612 (PA612) composites containing 10, 30, and 50 wt.% BF were prepared by melt compounding and micro‐injection molding. The effects of BF loading on fiber length, melt flow, mechanical properties, fracture morphology, and thermal behavior were examined. Tensile modulus, flexural strength, and notched Izod impact strength increased continuously with BF content, whereas tensile strength increased modestly at 10 wt.% BF (+10%) but rose substantially at 30 and 50 wt.% BF (+118% and +184%). Elongation at break decreased to 5%–9%, indicating a more brittle‐like tensile response. Mean recovered fiber lengths were 616 ± 153, 557 ± 136, and 552 ± 117 μm for BF10, BF30, and BF50, respectively. The melt volume‐flow rate (MVR) of BF50 was 87.39 cm 3 /10 min, compared with 83.26 cm 3 /10 min for neat PA612. BF increased the crystallization temperature from 182.0°C to 188.2°C–188.8°C. Whole‐composite T 5% values (424.9°C–430.4°C) exceeded that of neat PA612 (417.8°C). T max values of the BF composites (461.3°C–462.2°C) also exceeded that of neat PA612 (457.0°C). Fracture surfaces showed exposed fibers and pullout cavities, but no obvious fiber fracture was observed. These results identify interfacial engineering and high‐loading flow behavior as priorities for further development.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Enhancement of Thermal and Mechanical Properties of Polyamide 612 via Incorporation of Basalt Fiber — Science Skim