Filler-Geometry-Dependent Crystallinity, Melt Flow, and Mechanical Response of Glass-Filled PHBV + PBAT + TPS Composites.
Magdalena Pantoł, Klaudia Porzezinska, Krzysztof Nowik, Ewa Borucinska-Parfieniuk, Mehmet Aladag, Adrian Dubicki, Krzysztof J Kurzydłowski, Izabela B Zgłobicka
Faculty of Mechanical Engineering, Bialystok University of Technology, Wiejska 45C, 15-351 Bialystok, Poland.
Key points
From the paper's conclusion- Overall, the two filler geometries exhibited distinct relationships among apparent melt flowability, crystalline organization, quantitative microstructural descriptors, and mechanical response.
Abstract
The structural, processing, and mechanical response of a multiphase poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV)/poly(butylene adipate-co-terephthalate) (PBAT)/thermoplastic starch (TPS) matrix to two distinct glass fillers was investigated. Glass fibers and hollow glass spheres were incorporated by melt compounding and injection molding, while the unfilled blend served as the reference. Differential scanning calorimetry, X-ray diffraction, melt-flow-rate measurements, helium pycnometry, scanning electron microscopy with deep-learning-based segmentation, tensile, and Charpy impact tests were applied. At higher filler contents, the composite-level XRD-based crystallinity index decreased to approximately 47%, whereas the Scherrer-derived PHBV (110) coherent-domain size remained within approximately 21-24 nm. Preferred orientation, assessed independently from the PHBV reflection-intensity ratio, varied with filler type and content. Glass fibers progressively reduced melt flow and were associated with an increase in tensile modulus from 2.06 to 3.45 GPa and maximum tensile stress from 23.46 to 27.32 MPa at the highest investigated fiber content. Hollow glass spheres produced a non-monotonic melt-flow response, while the reduction in tensile performance at higher contents coincided with decreasing interparticle spacing and increasing specific external polymer-glass interfacial area. Within the analyzed SEM fields, no pronounced filler-rich clustering was evident. Notched specimens remained brittle, whereas unnotched specimens retained impact strength above 10 kJ × m-2. Overall, the two filler geometries exhibited distinct relationships among apparent melt flowability, crystalline organization, quantitative microstructural descriptors, and mechanical response.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Disintegration Behavior in Industrial Conditions of Poly(lactic acid)/Poly(hydroxybutyrate-co-valerate) Blends.ACS omega · 2026
- Synergistic effects of PHAs and biomass fillers on the thermal, rheological, and mechanical properties of biocompositesComposites Part A Applied Science and Manufacturing · 2025
- Rheology-Guided PHB/PBAT/MgO Nanocomposites for FDM Printing with Balanced Mechanical and Degradation Performance.ACS omega · 2026
- Structure-Property-Degradation Relationships in PHBV Biocomposites Filled with Cellulose, Walnut Shell, and Wood Fibres.Materials (Basel, Switzerland) · 2026
- Crystallization- and Shear-Induced Structural Evolutions in Polyhydroxyalkanoate-Blend FoamsIndustrial & Engineering Chemistry Research · 2026
- Thermal, Mechanical, and Rheological Properties of PLA/PHB Biocomposites Reinforced with Alkaline-Treated Hemp Fibers and GranulesChemEngineering · 2025