Materials (Basel, Switzerland)

Structure-Property-Degradation Relationships in PHBV Biocomposites Filled with Cellulose, Walnut Shell, and Wood Fibres.

Patrycja Szydłowska, Patrycja Bazan, Stanisław Kuciel

Faculty of Materials Engineering and Physics, PK Krakow University of Technology, Jana Pawła II 37, 31-864 Kraków, Poland.

Key points

From the paper's conclusion
  • PHBV composites incorporating 10 and 20% by weight of cellulose, walnut shell particles, or wood filler were produced under consistent extrusion and injection-moulding conditions for comparative analysis.

Abstract

PHBV composites incorporating 10 and 20% by weight of cellulose, walnut shell particles, or wood filler were produced under consistent extrusion and injection-moulding conditions for comparative analysis. The study assessed morphology, wettability, water absorption, mechanical properties at 23 and 80 °C, thermal decomposition, and alterations in mechanical properties following exposure to a detergent solution at 60 °C. Among the mean values reported, PHBV 20W exhibited the highest modulus at 23 °C (7403 MPa), while PHBV 10C demonstrated the highest impact strength (8.9 kJ/m2). At a filler content of 20% by weight, the tensile strength was observed to be lower than that of the matrix. After 35 days, water absorption varied from 1.3% for PHBV to 14.7% for PHBV 20W. Thermogravimetric analysis (TGA) results revealed that the direction of the shift in the temperature at 5% mass loss was filler-dependent, with values ranging from 229.2 to 272.2 °C, compared to 267.2 °C for PHBV. Exposure to detergent resulted in reductions in strength and elongation, with PHBV 20R and 20W experiencing a marked decrease in modulus.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers