Effect of Immediate Thermal Exposure on the Surface Mechanical Performance of Polyurethane-Coated Oak Wood and Visible 3D-Printed Furniture Components.
Gabriela Slabejová, Jozef Fekiač, Lukáš Adamčík, Zuzana Vidholdová
Department of Furniture and Wood Products, Faculty of Wood Sciences and Technology, Technical University in Zvolen, T. G. Masaryka 24, 96001 Zvolen, Slovakia. · Department of Woodworking, Faculty of Wood Sciences and Technology, Technical University in Zvolen, T. G. Masaryka 24, 96001 Zvolen, Slovakia.
Key points
From the paper's conclusion- This study investigated the effect of short-term exposure to 60 °C for 1 h on the surface mechanical properties of a pigmented polyurethane coating applied to oak wood and 3D-printed PLA, ABS-T and PET-G components.
Abstract
A polyurethane coating represents the conventional solution for protecting and finishing visible wooden furniture surfaces. However, the increasing use of additive manufacturing has introduced visible 3D-printed polymer components whose surface mechanical performance is relevant to their application in furniture. This study investigated the effect of short-term exposure to 60 °C for 1 h on the surface mechanical properties of a pigmented polyurethane coating applied to oak wood and 3D-printed PLA, ABS-T and PET-G components. Specimens were evaluated under laboratory conditions (20 °C) and immediately after exposure to 60 °C, while their surfaces remained at an elevated temperature. Impact resistance, abrasion resistance, and scratch resistance using a tungsten carbide tip were determined according to the relevant standards, and the surface damage was assessed by visual inspection and digital microscopy. The polyurethane coating exhibited the smallest impact indentation diameter but showed earlier crack initiation and lower abrasion resistance than the 3D-printed polymers. Among the investigated polymers, ABS-T provided the most balanced combination of impact resistance, abrasion resistance and surface hardness, whereas PLA exhibited the greatest dimensional changes after exposure to 60 °C. Microscopic analysis revealed surface defects that were not detectable by visual inspection, demonstrating the value of digital microscopy for detecting subtle surface damage. The results indicate that ABS-T is a promising material for visible furniture components exposed to short-term elevated temperatures, while PET-G should be used with caution in applications exposed to radiant heat or direct sunlight.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Investigation of Mechanical and Surface Properties of 3D-Printed Parts Aged Under Different Conditions (Coolant and Xenon Arc).Polymers · 2026
- Influence of 3D-Printing system on the mechanical and surface properties of a 3D-Printed denture base resin.Journal of applied biomaterials & functional materials · 2026
- Tribological Performance of FFF-Printed PLA and PLA-Wood Parts: The Effects of Infill Architecture, Heat Treatment, and Water Absorption.Polymers · 2026
- Effect of Printing Orientation and Post-Curing Time on the Mechanical Properties of 3D-Printed Denture Base ResinJournal of Functional Biomaterials · 2025
- Microstructure and Mechanical Performance of 3D-Printed Carbon Fibre—PLA-PHA CompositesPolymers · 2026
- Comparison of mechanical and optical properties of 3D printed denture bases.The Journal of prosthetic dentistry · 2026