From the paper's conclusion- The findings indicate that the best-performing infill architecture among the investigated configurations was the rectilinear pattern at an 80% infill density, which exhibited the lowest volumetric wear loss among all printing configurations.
Abstract
Polymer components fabricated via fused filament fabrication (FFF) are frequently exposed to friction and wear under diverse environmental conditions in various engineering applications. The tribological performance of these components is influenced by both the printing parameters employed during fabrication and subsequent post-processing and service conditions. Previous studies have generally investigated the effects of printing parameters or post-processing steps separately. However, a comprehensive evaluation of in-service performance requires the sequential consideration of these factors. This study aimed to evaluate the tribological performance of FFF-printed PLA and PLA-Wood specimens through a sequential approach considering the infill architecture, heat treatment, and subsequent water absorption. The findings indicate that the best-performing infill architecture among the investigated configurations was the rectilinear pattern at an 80% infill density, which exhibited the lowest volumetric wear loss among all printing configurations. The best-performing heat treatment conditions varied by material and were determined to be 90 °C for 15 min for PLA and 90 °C for 45 min for PLA-Wood, reducing volumetric wear loss from 17.97 to 14.32 mm3 (approximately 20%) and 24.92 to 22.36 mm3 (approximately 10%), respectively. Moreover, water absorption largely eliminated the heat-treatment-induced improvement in PLA, with volumetric wear loss increasing to 17.93 mm3, whereas the improvement was substantially retained in PLA-Wood, which exhibited a wear loss of 22.67 mm3 after water absorption. Overall, the findings demonstrate that improvements in wear resistance achieved through processing may not be equally retained after subsequent environmental exposure and that this response depends on the material composition.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Tribo-mechanical performance and microstructural characterization of FDM printed PLA and ABS componentsJournal of Materials Research and Technology · 2026
- Experimental Investigation into the Influence of Infill Density, Print Pattern, and Built-Up Direction on the Flexural Strength of FFF-Manufactured PLA ComponentsJournal of Manufacturing and Materials Processing · 2026
- Mechanical Parameters and Microstructural Evolution of FDM-Printed PLA and PLA+CF Under Variable Infill Architecture and Lubricant ExposurePolymers · 2025
- Effects of Pressurized Water Aging on Reciprocating Friction and Wear of FDM 3D-Printed PLA and Glass Fiber Reinforced PLA CompositesPolymers · 2026
- Enhancing the Performance of FFF-Printed Parts: A Review of Reinforcement and Modification Strategies for Thermoplastic PolymersMaterials · 2025
- Optimizing the Mechanical Performance of 3D-Printed PLA, ABS, and PETG Through Infill Density and PatternJournal of Manufacturing and Materials Processing · 2026