  • Background: The aim of this in vitro study was to compare the cyclic fatigue resistance and fractured fragment length of three nickel-titanium (NiTi) rotary systems of identical tip size and taper (25/.06).

Abstract

Background: The aim of this in vitro study was to compare the cyclic fatigue resistance and fractured fragment length of three nickel-titanium (NiTi) rotary systems of identical tip size and taper (25/.06). NiTi rotary instruments fracture unpredictably in curved canals, and no cyclic fatigue data have been published for either the Endo Magic All in One or the Denco Pro-Flexi system; this study provides the first independent fracture data for both, benchmarked against the established One Curve Mini. Methods: A total of 60 instruments (n= 20 per group) of One Curve Mini 25/.06, Denco Pro-Flexi 25/.06, and Endo Magic All in One 25/.06 were tested. Cyclic fatigue testing was performed in an artificial canal within a stainless-steel block (60° curvature angle, 5 mm radius of curvature, 1.5 mm internal diameter) in distilled water at 35 ± 1 °C. Instruments were rotated at 300 rpm until fracture. The number of cycles to failure (NCF) was calculated, fragment lengths were measured with a digital caliper, and cross-sectional geometry was evaluated by scanning electron microscopy (SEM). Data were analysed using the Kruskal–Wallis and Dunn’s tests (α = 0.05). Results: Significant differences were found among the groups for both NCF and fragment length (p < 0.001). The highest NCF was recorded for Endo Magic All in One (9165.50 ± 2049.58), followed by One Curve Mini (3007.50 ± 470.79) and Denco Pro-Flexi (2023.00 ± 1134.43); all pairwise comparisons were significant. Fragments in the Denco Pro-Flexi group were significantly longer (7.51 ± 1.05 mm). SEM revealed circular, triple-helix, and square cross-sections for Endo Magic All in One, One Curve Mini, and Denco Pro-Flexi, respectively. Conclusions: Instruments identical in tip size and taper differed up to 4.5-fold in cyclic fatigue resistance, so comparable fracture risk cannot be assumed from these specifications alone; fragment length data further indicate that the least resistant system also separates at a level that complicates retrieval. The systems differed in cross-sectional geometry and in the alloy processing reported by their manufacturers; determining the relative contribution of these factors will require metallurgical characterisation.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Cyclic Fatigue Resistance and Fractured Fragment Length of Three NiTi Rotary Systems: An In Vitro Comparison — Science Skim