Performance Evolution and Microstructure Optimization of Recycled Fine Aggregate Rapid-Hardening Sulfoaluminate Cement Mortar by Nano-SiO2 Surface Modification.
Meinan Wang, Shuo Liu, Cong Zhang, Yaning Wu, Liang Wang, Tieming Guo
College of Civil Engineering & Architecture, Qingdao Agricultural University, Qingdao 266109, China. · Qingdao Branch of Tongyuan Design Group Co., Ltd., Qingdao 266001, China.
Key points
From the paper's conclusion- Therefore, 2% can be determined as the optimal NS concentration which can provide a theoretical basis for high-value resource recycling of recycled fine aggregates in SAC mortar.
Abstract
In this study, rapid-hardening sulfoaluminate cement (SAC) was used as cementitious material, and recycled fine aggregates (RFAs) were surface pretreated by immersion in nano-SiO2 (NS) suspensions. NS-modified SAC recycled fine aggregate mortars were prepared at three cement-sand ratios (1:1, 1:2 and 1:3) to systematically investigate the regulatory effects of NS concentrations (0%, 1%, 2% and 3%) on macroscopic performance, hydration products and interfacial microstructure. Multi-scale characterizations, including XRD, TG-DTG, SEM-EDS and microhardness tests, were carried out. The testing results show that appropriate NS can optimize SAC hydration by heterogeneous nucleation and the pozzolanic reaction. At a cement-sand ratio of 1:1, the compressive and flexural strengths gradually increase as the NS concentration rises from 0% to 2%. Compared with the control group, the 28 d compressive and flexural strength are enhanced by 19.5% and 16.6%, respectively, the drying shrinkage decreases by 8.0%, and carbonation resistance is obviously improved. Meanwhile, the formation of AFt is promoted, amorphous C-S-H gel accumulates continuously, and the content of Ca(OH)2 is gradually consumed by the pozzolanic reaction of NS. For specimens modified with 2% NS, the maximum microhardness reaches 1326 HV, which greatly benefits the mechanical properties of mortar. However, further increasing the NS concentration to 3% triggers nanoparticle agglomeration and reduces effective reactive silica, leading to a decline in hydration products, deteriorated interfacial compactness and reduced mechanical performance. Therefore, 2% can be determined as the optimal NS concentration which can provide a theoretical basis for high-value resource recycling of recycled fine aggregates in SAC mortar.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- RSM optimized mechanical performance and chemical durability of nano silica, nano alumina fiber reinforced alkali activated mortarScientific Reports · 2026
- Effects of Nano-SiO2 on the Pore Structure and Crack Behavior of Basalt Fiber-Reinforced Coal Gangue-Slag Geopolymer Concrete.Materials (Basel, Switzerland) · 2026
- Performance Analysis of Cement Mortar Modified with Nano-Silica and Nano-AluminaBuildings · 2026
- Efficient stabilization of dredged sediment by combining nano-modification and low-carbon supersulfated cementJournal of Rock Mechanics and Geotechnical Engineering · 2025
- Nanomodified Low‐Carbon Recycled Aggregates Concrete with Enhanced Durability Performancece/papers · 2026
- Sustainable enhancement of chemical durability and microstructural stability in cement mortar incorporating sodium silicate–silica fume treated recycled fine aggregateScientific Reports · 2026