RSM optimized mechanical performance and chemical durability of nano silica, nano alumina fiber reinforced alkali activated mortar
Mahmood Hunar Dheyaaldin, Mohammad Ali Mosaberpanah, Dler H Kadir, Gökhan Kaplan, Mustafa Özakça
American University in Dubai · Cyprus International University
Key points
From the paper's conclusion- The results demonstrate that alkali-activated mortars provide a strong and environmentally sustainable alternative to conventional cement-based systems, highlighting the efficiency and practical potential of this approach.
Abstract
This study aims to optimize the mechanical performance, durability, and environmental sustainability of alkali-activated mortars (AAM) incorporating nano-silica (NS), nano-alumina (NA), and polypropylene fiber (PPF). A three-factor, three-level Central Composite Design (CCD) within the Response Surface Methodology (RSM) framework was employed, generating 17 experimental mixtures prepared using fly ash (FA) and ground granulated blast-furnace slag (GGBS) as binder materials. The maximum compressive strength of 82 MPa was achieved in the mixture containing 2% NA, while the maximum flexural strength (12 MPa) was recorded in the mixture containing 1% NS and 0.5% PPF. ANOVA results confirmed the statistical significance of the developed models, with R² = 0.984 and R² = 0.977 for compressive and flexural strength, respectively. Nano-alumina produced a greater increase in strength than NS, and the combination of both nanomaterials enhanced the density of the microstructure through the formation of C-(A)-S-H and N-A-S-H gels. The incorporation of PPF improved durability by preventing microcrack formation and enhancing resistance to acidic and saline environments. For example, specimens containing 2% NS and 2% NA demonstrated more than 20% higher residual strength under sulfuric acid exposure compared with reference specimens. Scanning Electron Microscopy (SEM) analyses showed that the nanomaterials accelerated early strength development by filling micro-voids and creating a more homogeneous matrix structure. A CO₂ emission analysis indicated that the optimized AAM mixture emits approximately 607.4 kg CO₂/m³, representing a reduction of about 26%. The results demonstrate that alkali-activated mortars provide a strong and environmentally sustainable alternative to conventional cement-based systems, highlighting the efficiency and practical potential of this approach.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Performance Evolution and Microstructure Optimization of Recycled Fine Aggregate Rapid-Hardening Sulfoaluminate Cement Mortar by Nano-SiO2 Surface Modification.Nanomaterials (Basel, Switzerland) · 2026
- Effect of Sodium Hydroxide Molarity and Nano-Alumina on Mechanical and Durability Properties of Alkali-Activated MortarJournal of Composites Science · 2026
- Performance Analysis of Cement Mortar Modified with Nano-Silica and Nano-AluminaBuildings · 2026
- Mechanical and durability performance of reactive powder concrete under acidic conditions: Role of nano‐silica, pozzolanic admixtures, and curing methodsStructural Concrete · 2026
- Role of meso-porous MgAl-LDH nanorods in the hydrothermal alkali activation of slag binders: Mechanical integrity and thermal stabilityJournal of Materials Research and Technology · 2026
- Assessment of the Physical and Mechanical Properties of Autoclaved Aerated Concrete (AAC) Incorporated with Sisal Fibers and Nano-Aluminum ParticlesThe Open Construction and Building Technology Journal · 2026