Calcium Chloride Activation of Acid-Washed Sewage Sludge Ash: Hydration Mechanism and Performance as a Supplementary Cementitious Material.
Weiwei Zhu, Yi Ren, Yaxin Xiao, Shaoyu Du, Xiaoli Xie, Kao Chen
School of Materials and Environment, Guangxi Key Laboratory of Advanced Structural Materials and Carbon Neutralization, Guangxi Engineering Research Center for Advanced Materials and Intelligent Manufacturing, Guangxi Minzu University, Nanning 530105, China. · School of Civil Engineering, Guangxi Polytechnic of Construction, Nanning 530007, China.
Key points
From the paper's conclusion- To this end, this paper proposes to remove phosphorus from incinerated sewage sludge ash (ISSA) by the acid washing process, and, in response to the problem of reduced volcanic ash activity in acid-washed sewage sludge ash (ASSA), calcium chloride (CaCl2) is added as an activator to explore the optimal process and hydration mechanism for enhancing ASSA activity.
Abstract
Due to the fact that municipal sludge incineration generates a large amount of toxic sewage sludge ash (SSA), cement solidification is becoming an efficient harmless treatment method. However, the large amount of phosphorus in sludge ash can delay the setting time of cement pastes and lead to a decrease in its later strength. Moreover, as an important non-renewable resource, the recycling and utilization of phosphorus is also a current research hotspot. To this end, this paper proposes to remove phosphorus from incinerated sewage sludge ash (ISSA) by the acid washing process, and, in response to the problem of reduced volcanic ash activity in acid-washed sewage sludge ash (ASSA), calcium chloride (CaCl2) is added as an activator to explore the optimal process and hydration mechanism for enhancing ASSA activity. This study removed phosphorus from calcined SSA (800 °C, 2 h) via acid washing (0.3 mol/L H2SO4, L/S = 10:1, 2 h) to obtain ASSA, and used CaCl2 as an activator to improve its pozzolanic activity. Different CaCl2 dosages (1-3%) were tested for paste setting time, 3/7/28 d compressive strength, and characterized by hydration heat, XRD, SEM, etc. Experimental results indicated that the synergistic addition of 2 wt.% CaCl2 and 20 wt.% ASSA shortened the initial and final setting times by 38% and 23% to 142 min and 289 min, respectively. Meanwhile, the compressive strength at 28 days was improved by 24%, with a final strength value of 42 MPa. Microanalysis revealed abundant Friedel's salt formation and a denser structure (fine mesopores 60%, coarse mesopores 26%), confirming CaCl2 effectively activates ASSA for cement admixture use.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of sewage sludge ashes on the performance of cementitious compositesMaterialia · 2026
- Enabling the High-Volume Utilization of Iron-Rich Sewage Sludge Ash in Cement: The Role of Curing Temperature in Microstructure and Performance Enhancement.ACS omega · 2026
- Sewage sludge ash in concrete: a comprehensive review on properties, performance, and environmental sustainabilityDiscover Civil Engineering · 2026
- Upcycling of municipal solid waste incineration bottom ash (MSWIBA) into a value-added supplementary cementitious material: Effect of Ca(OH)2 and temperatureConstruction and Building Materials · 2025
- Carbonation Pretreatment of Slag for Improving the Rheological Behavior and Sustained Grouting Performance of Alkali-Activated Grouting MaterialsBuildings · 2026
- Multi-Scale Investigation on the Hydration and Microstructure of Portland Cement Blended with Inorganic Softening Sludge.Materials (Basel, Switzerland) · 2026