Micromachines

Forging-Induced Microstructural Heterogeneity and Localized Thermal Resistance in W-Cu Heat Sinks for High-Power Semiconductor Laser Bar Packaging.

Guofeng Yang, Jin Zhang, Chi Hu, Yao Li, Shenjiang Wu

School of Opto-Electronic Engineering, Xi'an Technological University, Xi'an 710021, China.

Key points

From the paper's conclusion
  • The results indicate that microstructural uniformity and interfacial integrity, rather than average thermal conductivity, control device-level thermal management, and that forging parameters must be optimized to preserve continuous heat flow pathways.

Abstract

Tungsten-Copper (W-Cu) alloys are widely used as heat spreaders in high-power semiconductor laser bar packages because of their high thermal conductivity and tailorable thermal expansion. Here, we show that unidirectional forging of 70W-30Cu changes the bulk thermal conductivity by less than 5% but reduces the output power of packaged laser bars by approximately 20% at the same injection current. The degradation is not explained by bulk conduction alone. Forging introduces surface pits, local softening of the Cu network, and interfacial damage that increase contact and constriction resistance along the die-attach heat path, creating localized thermal bottlenecks. A combined analysis of thermal diffusivity, heat capacity, electrical conductivity, hardness, and an illustrative finite-difference thermal model shows that an effective conductivity of 2 W m-1 K-1 raises the peak temperature, despite an unchanged bulk conductivity. The results indicate that microstructural uniformity and interfacial integrity, rather than average thermal conductivity, control device-level thermal management, and that forging parameters must be optimized to preserve continuous heat flow pathways.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers