Effect of Proton Irradiation Temperature on the Surface Degradation of High-Purity Tungsten
Anastassiya Tarapeyeva, Lyubov Dikova, Tamara Aldabergenova, Sergey Kislitsin, Irina Tazhibayeva, Igor Sokolov, Gainiya Zhanbolatova, Baurzhan Chektybayev
Key points
From the paper's conclusion- Irradiation at room temperature produced unruptured blisters, predominantly 10–20 μm in size; annealing at 873–1073 K reduced their total number while increasing the fraction of larger blisters (20–25 μm and above); and annealing at 1273 K fully dissolved the blisters without surface exfoliation, recovering microhardness to its initial level.
Abstract
Tungsten is regarded as a primary candidate for plasma-face material for internals of ITER and, possibly, other thermonuclear installations. This article presents the investigation results of the effect of low-energy proton irradiation temperature on the degradation of the structure and properties of ITER-grade tungsten. High-purity tungsten (99.94 wt.%) was irradiated with 350 keV protons to a fluence of 5 × 1017 cm−2 at room temperature and at 773 K (UKP-2-1 accelerator, Institute of Nuclear Physics, Almaty), followed by isochronal annealing at 873–1273 K. Structure and properties were examined through X-ray diffraction, scanning electron microscopy, atomic force microscopy, and microhardness measurements. Irradiation at room temperature produced unruptured blisters, predominantly 10–20 μm in size; annealing at 873–1073 K reduced their total number while increasing the fraction of larger blisters (20–25 μm and above); and annealing at 1273 K fully dissolved the blisters without surface exfoliation, recovering microhardness to its initial level. Irradiation at 773 K caused blister appearance and burst during irradiation process; predominant blister size was 3–5 μm; subsequent annealing produced second-generation blisters at the sites of the primary ones. After annealing at 1273 K, only erosion spots and second-generation blisters were left on the surface; microhardness recovered also.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Comparative investigation of temperature-dependent defect evolution and irradiation hardening in CVD and ITER-like tungstenNuclear Fusion · 2026
- Radiation damage in tungsten under high-energy He-ion irradiationCommunications Materials · 2026
- Temperature-Dependent Irradiation-History Effects in Tungsten Under Sequential Helium and Hydrogen Plasma Exposure.Materials (Basel, Switzerland) · 2026
- Study on radiation damage of tungsten-based targets induced by deuterium ions.PloS one · 2026
- Correlation Between Radiation Damage Evolution and Mechanical Properties of Fe-Irradiated Tungsten.Materials (Basel, Switzerland) · 2026
- Microstructural and Mechanical Characterization of W-3Re Coatings on TZM Produced by Vacuum Plasma SprayingApplied Sciences · 2026