Temperature-Dependent Irradiation-History Effects in Tungsten Under Sequential Helium and Hydrogen Plasma Exposure.
Zarina Satbayeva, Bauyrzhan Rakhadilov, Yerasyl Naimankumaruly, Yernar Turabekov, Yelaman Batanov
"PlasmaScience" LLP, Ust-Kamenogorsk 070000, Kazakhstan.
Key points
From the paper's conclusion- Overall, the results indicate that the tungsten response under the present sequential protocol depends on both temperature and exposure history, and that structural convergence at elevated temperature does not necessarily correspond to equivalent hydrogen-release behavior.
Abstract
Tungsten plasma-facing components in fusion devices may experience sequential exposure to helium and hydrogen, making irradiation history an important factor in their subsequent structural and hydrogen-release behavior. This study investigated polycrystalline tungsten exposed to He-only, H2-only, and sequential He → H2 plasmas at 700, 900, 1100, and 1300 °C. Surface and cross-sectional scanning electron microscopy, X-ray diffraction, instrumented indentation, and thermal desorption spectroscopy (TDS) were used to characterize the resulting changes. SEM observations showed that the largest differences among the H2-only, He-only, and sequential He → H2 exposure conditions occurred at 1100 °C, whereas predominantly grain-scale surface morphology was observed for all three conditions at 1300 °C. The bcc-W structure was retained under all investigated conditions, with no detectable secondary crystalline phases. The apparent coherent diffraction domain size, estimated from the W(110) reflection using the Scherrer equation, increased monotonically with irradiation temperature, from approximately 48-55 nm at 700 °C to approximately 126 nm at 1300 °C. At 1100 °C, the H2-only specimen exhibited a larger apparent coherent diffraction domain size than the He-containing specimens. The nanomechanical response also depended on temperature and exposure history. TDS revealed distinct high-temperature hydrogen-desorption behavior for the sequential He → H2 specimens, particularly at 1100 and 1300 °C. Overall, the results indicate that the tungsten response under the present sequential protocol depends on both temperature and exposure history, and that structural convergence at elevated temperature does not necessarily correspond to equivalent hydrogen-release behavior.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Proton Irradiation Temperature on the Surface Degradation of High-Purity TungstenMetals · 2026
- Radiation damage in tungsten under high-energy He-ion irradiationCommunications Materials · 2026
- Effects of uniaxial strain and free hydrogen/helium atoms on helium bubble coalescence in tungsten divertorNuclear Fusion · 2026
- Correlation Between Radiation Damage Evolution and Mechanical Properties of Fe-Irradiated Tungsten.Materials (Basel, Switzerland) · 2026
- Temperature- and Geometry-dependent grain boundary transport of deuterium in tungsten by hydrogenographyNuclear Fusion · 2026
- Grain boundary effects on surface modifications of tungsten under fusion-relevant helium plasma irradiation: Coarse-grained vs. Nano-grained microstructuresNuclear Fusion · 2026