Microstructural Evolution and Mechanical Property Changes of Al/Mg/Al Laminated Composites Under Different Annealing Temperatures
Xingwang Duan, Yingjie Huo, Bin Fu, Zhuowu Guo, Zhiyong Wang, Huanxin Liu
Key points
From the paper's conclusion- In summary, favorable comprehensive performance is obtained under the annealing condition of 350 °C/60 min, with σs/σb of 0.733, an IE of 3.27 mm and a peeling strength of 4.1 N/mm.
Abstract
To investigate the effect of annealing temperature on interface evolution, microstructure and the mechanical properties of Al/Mg/Al laminated composites (LMCs), LMCs fabricated by flat rolling at 400 °C were annealed at 200, 250, 300, 325, 350 and 375 °C for 60 min. Scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), X-ray diffraction (XRD), electron back-scatter diffraction (EBSD), transmission electron microscopy (TEM), as well as tensile, cupping, peeling and hardness tests were employed to characterize their interfacial structure, microstructure and mechanical properties. With increasing annealing temperature, the interface gradually transforms from mechanical interlocking to metallurgical bonding, and the intermetallic compound (IMC) layer thickens continuously. Excessive elemental interdiffusion causes interfacial embrittlement at 375 °C. The Mg layer undergoes recovery, recrystallization, and grain growth, accompanied by changes in crystallographic texture. In contrast, the Al layer possesses a higher recrystallization temperature; it maintains a deformed microstructure at low temperatures and exhibits prominent recrystallization only at 350 °C. The dislocation density of both layers decreases first and then increases, reaching the minimum value at 350 °C. In terms of mechanical properties, the yield strength (YS) decreases monotonically with rising annealing temperature, and the yield-to-tensile ratio (ratio of yield strength to ultimate tensile strength, σs/σb) declines correspondingly. The work-hardening exponent reaches a peak value of 0.291 at 350 °C. Elongation (EL) increases first and then fluctuates at a high level (10.2% at 350 °C). The peeling strength varies in a non-monotonic trend: it presents the maximum value of 12.3 N/mm at 200 °C, drops to the minimum of 1.1 N/mm at 325 °C, and rebounds to 4.1 N/mm at 350 °C and 8.1 N/mm at 375 °C. For stamping formability, the Erichsen cupping index (IE) is the lowest (2.12 mm) at 200 °C and stabilizes within the range of 3.15–3.31 mm above 250 °C. In summary, favorable comprehensive performance is obtained under the annealing condition of 350 °C/60 min, with σs/σb of 0.733, an IE of 3.27 mm and a peeling strength of 4.1 N/mm. This condition exhibits good comprehensive formability and provides an experimental basis for the annealing-process design of LMCs.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Annealing-induced strengthening in hetero-structured Mg alloy laminates with gradient Al contentJournal of Magnesium and Alloys · 2025
- Microstructure and Mechanical Properties of Immiscible Ti/Mg Laminated Composite Plates After Low-Temperature AnnealingMetals · 2026
- Short-time annealing achieves interfacial equilibration and strength-ductility synergy in ultrasonic additive manufactured Ti/Al laminated compositesMaterials Science and Engineering A · 2026
- Synergistic control of microstructure and plasticity in hot-rolled Ti/Mg laminated composite plates by matrix composition and interfacial oxidationJournal of Materials Research and Technology · 2026
- A Perspective on Mg/Al Laminated Metal Composites.Materials (Basel, Switzerland) · 2026
- Interfacial microstructure and dynamic compressive behavior of explosively welded TA2/AZ31B/7075Al multilayer compositesJournal of Materials Research and Technology · 2026