Microstructure and Mechanical Properties of Immiscible Ti/Mg Laminated Composite Plates After Low-Temperature Annealing
Bin Yang, Yunchang Guo, Shenghao Lu, Chao Yu, Caiyi Liu, Silvia Barella, Andrea Gruttadauria, Marco Belfi,
Key points
From the paper's conclusion- Annealing at 200 °C was identified as the preferred annealing temperature, offering a viable pathway to strength–ductility synergy in immiscible lightweight Ti/Mg laminated composite plates.
Abstract
Achieving strength–ductility synergy in immiscible Ti/Mg laminated composites remains challenging, owing to the absence of metallurgical bonding and the limited slip systems of their hexagonal close-packed (HCP) structures. This study aims to achieve a favorable strength–ductility balance in immiscible Ti/Mg laminated composite plates via low-temperature annealing after hot-roll bonding. The results show that after post-rolling annealing at 200 °C, the bonding strength of the Ti/Mg composite interface increased from 48.74 MPa to over 80 MPa without the formation of obvious intermetallic compounds. In the Mg layer, complete recrystallization eliminated the shear bands, and pyramidal slip—exhibiting the highest Schmid factor—became the dominant strain-accommodation mode. In the Ti layer, recovery, rather than full recrystallization, prevailed. Concurrently, basal and pyramidal slip were co-activated to enable multi-slip load bearing. These complementary deformation modes, coordinated through the strengthened interface, promoted compatible deformation between the layers, in which the plastic flow of the Mg layer relieved local strain concentration in the Ti layer, resulting in a more than twofold increase in elongation with minimal loss of strength. Annealing at 200 °C was identified as the preferred annealing temperature, offering a viable pathway to strength–ductility synergy in immiscible lightweight Ti/Mg laminated composite plates.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Synergistic control of microstructure and plasticity in hot-rolled Ti/Mg laminated composite plates by matrix composition and interfacial oxidationJournal of Materials Research and Technology · 2026
- Annealing-induced strengthening in hetero-structured Mg alloy laminates with gradient Al contentJournal of Magnesium and Alloys · 2025
- Synergistic enhancement of strength and ductility in Mg-7Sn alloy through combined optimization of dual-texture and low-angle grain boundary structuresJournal of Magnesium and Alloys · 2026
- Microstructural Evolution and Mechanical Property Changes of Al/Mg/Al Laminated Composites Under Different Annealing TemperaturesMetals · 2026
- Ductilizing hot-rolled Ti6Al4V/Al composite via flash annealingJournal of Materials Research and Technology · 2026
- Breaking strength-ductility trade-off in magnesium alloy by semi-solid extrusion process: Multi-slip activation in “Bimodal Grain”Journal of Magnesium and Alloys · 2025