Effect of PTA Current on Microstructure, Phase Constitution, Hardness and Dry-Sliding Wear of Fe–Cr–C Layers Deposited on 35L Cast Steel
A. B. Shynarbek, Zarina Satbayeva, B. K. Rakhadilov, Duman Orynbekov, Ainur Zhassulan, Kuanysh Ormanbekov, Nurlat Kadyrbolat, Duman Askerzhanov
Shakarim University · Sarsen Amanzholov East Kazakhstan University
Key points
From the paper's conclusion- This study investigates plasma transferred arc (PTA) surfacing of 35L cast steel using a high-chromium Fe–Cr–C powder (PG-S27) and clarifies how the welding current (40–120 A) governs layer geometry, microstructure, phase constitution, hardness, and dry-sliding tribological behavior.
Abstract
Wear of crushing and grinding equipment components causes frequent maintenance and downtime; therefore, effective repair hardfacing routes are required to extend service life. This study investigates plasma transferred arc (PTA) surfacing of 35L cast steel using a high-chromium Fe–Cr–C powder (PG-S27) and clarifies how the welding current (40–120 A) governs layer geometry, microstructure, phase constitution, hardness, and dry-sliding tribological behavior. All deposits exhibited a dendritic–eutectic structure; increasing current led to dendrite coarsening, wider interdendritic regions, and deeper penetration/dilution. X-ray diffraction indicated an α-Fe matrix with chromium carbide phases (Cr7C3/Cr23C6), while the carbide-related signal decreased with higher current, consistent with enhanced dilution. The coatings showed a strong hardening effect compared with the substrate (~190 HV), reaching ~625–650 HV at 40–80 A and decreasing to ~556–589 HV at 100–120 A. In dry ball-on-flat sliding, the steady-state friction coefficient was nearly unchanged (μ ≈ 0.50–0.55) across all regimes; however, wear resistance depended strongly on current: the lowest wear was achieved at low-to-moderate currents (40–80 A), whereas higher currents (100–120 A) resulted in substantially increased material loss, approaching the substrate level. These results identify 40–80 A as the most favorable current window for obtaining wear-resistant PTA layers from PG-S27 on 35L steel.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructure and Wear Performance of Ni-Based Laser Cladded Coatings Reinforced with Different ZrC Contents on Structural SteelCoatings · 2026
- Improving the Wear Resistance of 40Cr Steel by Multi-Pass Laser Hardening: Effect of the Number of Passes on the Microstructure, Microhardness and Tribological PropertiesApplied Sciences · 2026
- Microstructure, Wear Resistance and Corrosion Resistance of FeNiCrMo, FeNiCrMo/WC and FeNiCrMo/WC-17Co Coatings Prepared by Laser Cladding: A Comparative StudyCrystals · 2026
- Laser cladding high wear and tribo-corrosion resistant Fe-based defect-free layers on nodular cast ironCeramics International · 2025
- Effect of Laser Cladding with Constant Specific Energy on the Hardness and Friction Properties of Stellite 21 Coatings on AISI 304 Stainless SteelCoatings · 2026
- Comparative Study of the Microstructure, Local Elemental Composition, Microhardness, and Dry-Sliding Friction Behavior of Co-Cr-W, Fe-Mn-C, and Fe-Cr-Ni-Mn GTAW Deposits on 09G2S SteelJournal of Manufacturing and Materials Processing · 2026