The Leaching of Valuable Metals (Li, Co, Ni, Mn, Cu) from Black Mass from Spent Lithium-Ion Batteries
Rorie Gilligan, Glen O’Malley, Aleksandar N. Nikoloski
Murdoch University
Key points
From the paper's conclusion- Near-complete (>99%) dissolution of lithium and cobalt was achieved by the leaching of black mass from spent (end-of-life) lithium-ion batteries (LiBs) using 4 M H2SO4 or HCl at 60 °C.
Abstract
Near-complete (>99%) dissolution of lithium and cobalt was achieved by the leaching of black mass from spent (end-of-life) lithium-ion batteries (LiBs) using 4 M H2SO4 or HCl at 60 °C. Raising the temperature to 90 °C did not increase the overall extraction of lithium or cobalt, but it increased the rate of extraction. At 60 °C, 2 M H2SO4 or 2 M HCl performed similarly to the 4 M H2SO4/HCl solution, although extractions were lower using 1 M H2SO4 or HCl (~95% and 98%, respectively). High extractions were also observed by leaching in low pulp density (15 g/L) at 60 °C with 2 M CH2ClCOOH. Leaching was much slower with hydrogen peroxide reductant concentrations below 0.5 mol/L, with cobalt extractions of 90–95% after 3 h. Pulp densities of up to 250 g/L were tested when leaching with 4 M H2SO4 or HCl, with the stoichiometric limit estimated for each test based on the metal content of the black mass. Extractions were consistently high, above 95% for Li/Ni/Mn/Cu with a pulp density of 150 g/L, dropping sharply above this point because of insufficient remaining acid in the solution in the later stages of leaching. The final component of the test work used leaching parameters identified in the previous experiments as producing the largest extractions, and just sulphuric acid. A seven-stage semi-continuous sulphuric acid leach at 60 °C of black mass from LiBs that had undergone an oxidising roast (2h in a tube furnace at 500 °C under flowing air) to remove binder material resulted in high (93%) extraction of cobalt and near total (98–100%) extractions of lithium, nickel, manganese, and copper. Higher cobalt extraction (>98%) was expected, but a refractory spinel-type cobalt oxide, Co3O4, was generated during the oxidising roast as a result of inefficient aeration, which reduced the extraction efficiency.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Non-aqueous leaching of critical metals from black mass of spent lithium-ion batteries using a reusable acidic organophosphorus extractantJournal of Environmental Management · 2025
- Metal Extraction and Solid-Phase Evolution During Ammoniacal Leaching of Spent LiCoO2 CathodesMetals · 2026
- Environmentally Friendly Separation of Lithium and Cobalt from Spent Li-ion Batteries Using Water and Organic Acid LeachingKorean Journal of Chemical Engineering · 2026
- Early-Stage Recovery of Lithium from Lithium-Ion Battery Black Mass in Pilot Scale Using Supercritical CO2ACS Sustainable Resource Management · 2026
- Recovery of Valuable Metals from Spent Lithium-Ion Batteries by Combining Reduction Roasting and Selective LeachingRecycling · 2026
- Comparative Reduction Roasting of Mn-Rich Spent NCM Black Mass After NaOH Pretreatment for Selective Metal Recovery: Self-Reduction, CO, and H2 PathwaysMetals · 2026