Comparative Reduction Roasting of Mn-Rich Spent NCM Black Mass After NaOH Pretreatment for Selective Metal Recovery: Self-Reduction, CO, and H2 Pathways
Liangqu Huang, Qianwen Yang, Chuan Chen, Hui Liu, Yuping Zhang
Key points
From the paper's conclusion- Among the three routes, CO reduction achieved the highest lithium recovery of 87.4% (relative to the lithium remaining in the NaOH-pretreated alkaline leaching residue; the lithium originally present in the Mn-rich spent NCM black mass is the denominator for the overall mass-balance basis) at 10% CO, 600 °C and 90 min, outperforming self-reduction (60.4%) and H2 reduction (60.7%).
Abstract
Coal-based reduction roasting is a widely used processing unit for recycling valuable metals (Li, Ni, Co, and Mn) from Mn-rich spent NCM black mass. However, solid carbon reductants require high temperatures (≥650 °C) and promote the formation of water-insoluble LiAlO2 via reactions between Li2O and Al-/F-bearing impurities. Herein, Mn-rich spent NCM black mass after mild NaOH leaching (1 wt%) was subjected to self-reduction, CO reduction, and H2 reduction, and the three routes were systematically compared. Thermodynamic calculations, XRD, and XPS were used to elucidate phase evolution and element migration. Among the three routes, CO reduction achieved the highest lithium recovery of 87.4% (relative to the lithium remaining in the NaOH-pretreated alkaline leaching residue; the lithium originally present in the Mn-rich spent NCM black mass is the denominator for the overall mass-balance basis) at 10% CO, 600 °C and 90 min, outperforming self-reduction (60.4%) and H2 reduction (60.7%). The superior performance of CO reduction is attributed to a synergistic effect between externally supplied CO and residual organics/graphite, which generates a controlled atmosphere that promotes Li2CO3 formation while suppressing LiAlO2 crystallization. Subsequent sulfuric acid leaching of the water-leaching residue enabled nearly complete recovery of Ni, Co, and Mn, with leaching efficiencies exceeding 99.9%. This work provides mechanistic insight and comparative process data for optimizing reduction roasting–water leaching routes for selective metal recovery from Mn-rich spent NCM black mass.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Recovery of Valuable Metals from Spent Lithium-Ion Batteries by Combining Reduction Roasting and Selective LeachingRecycling · 2026
- CO2-assisted selective lithium extraction and closed-loop regeneration of spent NCM cathodes toward cleaner battery recycling.RSC advances · 2026
- Selective lithium recovery from spent LiMn2O4 cathodes through carbothermic reduction.Waste management (New York, N.Y.) · 2026
- Synergistic Pyrolytic Recovery of Valuable Metals from Spent NCM Cathodes via MnCl2-Coffee Ground Co-TreatmentACS Sustainable Resource Management · 2026
- Thermodynamically self-limited reduction enables morphology-preserving selective delithiation for spent cathode recycling.Waste management (New York, N.Y.) · 2026
- Current Collector Augmented Reductive Dissolution of Spent Li-Ion Battery Black Mass for Regeneration of NMC622 CathodeACS Sustainable Chemistry & Engineering · 2026