Multiscale Chemical and Microstructural Characterisation of IF-WS2 Modified Anodic Coatings: From GD-OES Profiling to Local Wear Mechanisms

Joanna Korzekwa, Przemysław Kwolek, Wojciech J. Nowak, Krzysztof Krupa, Mateusz Niedźwiedź, Marek Bara

Key points

From the paper's conclusion
  • This study provides a multiscale investigation of the chemical depth architecture, micromechanical properties, and dry sliding tribological performance of nanoporous anodic Al2O3 coatings on EN AW-5251 aluminium alloy modified with inorganic fullerene-like tungsten disulphide (IF-WS2) nanoparticles.

Abstract

This study provides a multiscale investigation of the chemical depth architecture, micromechanical properties, and dry sliding tribological performance of nanoporous anodic Al2O3 coatings on EN AW-5251 aluminium alloy modified with inorganic fullerene-like tungsten disulphide (IF-WS2) nanoparticles. Two incorporation strategies were evaluated: an active ultrasonic-assisted method (method A) and a passive gravitational sedimentation method (method B). Point EDS analysis confirmed localized tungsten enrichment (up to 6.60 wt.%) within discrete surface agglomerates, contrasting with matrix-diluted bulk area averages. Qualitative Glow Discharge Optical Emission Spectrometry (GD-OES) depth profiling revealed an overall reduction in sulphur content across the coating volume (from ~4.0 wt.% to 1.2–1.7 wt.%), which is hypothesised to result from post-anodising sulphate leaching during suspension processing rather than altered oxide growth kinetics. ISO-compliant surface roughness evaluation (Ra, N = 342 profiles) revealed a statistically significant difference using the Kruskal–Wallis H-test (p = 0.0011), with post hoc Dunn’s testing confirming a significant roughness increase exclusively for method A. Ball-on-flat tribological tests (conducted under normal loads of 3.1–4.6 N over a sliding distance of 500 m) demonstrated a distinct load-dependent friction crossover: at 3.1 N, sliding resistance was controlled by initial surface roughness (Ra), whereas at 4.6 N, solid lubrication activation in method A reduced the median friction coefficient to µ = 0.75 (compared to 0.81 for reference Al2O3). Evaluation of Archard’s volumetric specific wear rate k (mm3/(N·m)) derived from n = 10 3D profilometric cross-sections per wear track according to ISO 20808:2016 revealed a fundamental discrepancy between friction reduction and volumetric wear resistance under high contact stress. These findings demonstrate that hydrodynamic forcing during incorporation allows tailored microstructural and tribological optimisation of self-lubricating anodic oxide composite coatings.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers