Study of tribological and corrosion behavior of AA6061–SiC–WS₂/WSe₂ hybrid composites using the taguchi method
Vijayasarathi Prabakaran, M Venkatasudhahar, Ravikumar Jayabal, Mary Nancy Flora Rayappan, A. Kumaravel, Karthikeyan Murugan
Vel Tech Rangarajan Dr. Sagunthala R&D Institute of Science and Technology · AMET University
Key points
From the paper's conclusion- Abstract The present research reports our work on the design of Al6061 based hybrid metal matrix composites which we have included silicon carbide (SiC), tungsten disulfide (WS₂) and tungsten selenide (WSe₂) to improve the mechanical, tribological, and corrosion resistance which is a requirement for brake rotors, piston rings, and sliding bearings.
Abstract
Abstract The present research reports our work on the design of Al6061 based hybrid metal matrix composites which we have included silicon carbide (SiC), tungsten disulfide (WS₂) and tungsten selenide (WSe₂) to improve the mechanical, tribological, and corrosion resistance which is a requirement for brake rotors, piston rings, and sliding bearings. Three composites Al6061, Al6061/14wt.%SiC/0.1wt.%WS₂, and Al6061/14wt.%SiC/0.1wt.%WSe₂ were fabricated using the stir casting technique. XRD analysis reported that the reinforcements are well distributed and present in all composites. Microhardness results indicated that the addition of reinforcements improved the composite performance, with Al6061/14 wt% SiC/0.1 wt% WSe₂ exhibiting the highest hardness. Experiments using sliding velocities of 0.5, 1.0, and 1.5 m/s and normal forces of 10, 20, and 30 N, analyzed via Taguchi L 27 and ANOVA, revealed that sliding speed was the dominant factor affecting wear rate and coefficient of friction (COF). The specific wear rate (3.228 × 10⁶ mm³/N·m) and lower COF of Hard SiC and lubricating WSe₂ of the Al6061/14wt%SiC/0.1wt%WSe₂ composite evidenced this. Corrosion studies showed that the composite exhibited a shift in corrosion potential (E corr ) from − 744 to − 663 mV, a decrease in corrosion current density (I corr ) from 12.7 to 4.8 µA/cm², and a corresponding increase in protection efficiency of 61.6%. The regression model showed strong reliability (R² = 0.98) and a 10.26% deviation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Wear and tribological analysis of graphite-reinforced Al6061-TiB2 hybrid composites fabricated by stir castingJournal of Materials Science Materials in Engineering · 2026
- Effect of the weight fraction of bagasse and aloe vera ash on the friction and sliding wear behavior of an Al6061 reinforced silicon carbide hybrid compositeDiscover Materials · 2025
- Comparative study on the morphology and tribological behaviour of Co/WS₂ , Co/WC, and hybrid Co/WC–WS₂ composite coatingsTransactions of the IMF · 2026
- Dry-Sliding Friction and Wear of Powder-Metallurgy AA6061 Composites with Multiscale TiB2–SiC ReinforcementLubricants · 2026
- Investigation of strength and microstructural evaluation of friction stir processed AA6061 alloy surface composite reinforced with tungsten carbide and nitinol particlesCanadian Metallurgical Quarterly · 2026
- Microhardness and Dry Sliding Wear Behaviour of Ultrasonically Stir-Cast Al7075 Hybrid Nano-Composites Reinforced with SiC, B4C and Al2O3Engineering Research Express · 2026