Fracture Damage Evolution of Stone Mastic Asphalt Mixtures Subjected to Salt Freeze–Thaw Cycles: A Multiscale Characterization Using SCB, AE, and DIC
Ziyi Zhao, Qinling Zhang, Haidong Ji, Kuixing Ren, Baocun Yang
Key points
From the paper's conclusion- Semi-circular bending (SCB) tests were integrated with acoustic emission (AE) and digital image correlation (DIC) to clarify the fracture damage evolution of SMA mixtures subjected to different numbers of salt freeze–thaw cycles.
Abstract
Salt freeze–thaw cycles can induce internal damage in SMA mixtures and weaken their fracture resistance, yet the relationship between internal damage evolution and localized deformation near the crack tip remains unclear. Semi-circular bending (SCB) tests were integrated with acoustic emission (AE) and digital image correlation (DIC) to clarify the fracture damage evolution of SMA mixtures subjected to different numbers of salt freeze–thaw cycles. For comparative analysis of AE responses, the loading process was divided into four operational intervals using 0.8Fmax as a reference on the pre-peak and post-peak branches. The SCB results showed that the fracture energy Gf, Mode I critical stress intensity factor KI, and flexibility index FI decreased by 72.0%, 57.5%, and 32.4%, respectively, after 20 cycles, while the crack path became increasingly localized. The SCB results are expressed as mean ± standard deviation based on three replicate specimens per conditioning level (n = 3). Welch’s one-way ANOVA showed significant overall differences among the five conditioning levels for Gf, KI, S, and FI (p < 0.05), and Games–Howell post hoc comparisons were used to examine pairwise differences. AE revealed that salt freeze–thaw cycling advanced the onset of internal damage and concentrated energy release near the peak load and after the peak load, while the relative proportions of tensile-type and shear-type AE events varied non-monotonically with the number of salt freeze–thaw cycles. DIC showed a substantial reduction in localized deformation, with the spatially averaged maximum horizontal strain Exx and mean normalized crack opening response decreasing by 71.71% and 69.45%, respectively, after 20 cycles, while crack opening remained concentrated near the L1 measurement location. The findings provide a reference for characterizing the multiscale fracture response of SMA mixtures under salt freeze–thaw conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure InclinationApplied Sciences · 2026
- Mechanical Response and Macro–Micro Damage Mechanisms of Sandstone Under Low‐Frequency Cyclic Disturbance After Freeze–Thaw CyclingFatigue & Fracture of Engineering Materials & Structures · 2026
- Mechanical behavior and multiscale damage evolution of filled fractured sandstone under freeze-thaw cycles.Scientific reports · 2026
- Mechanical response and failure precursors of sandstone under freeze-thaw cycling with varying saturationInternational Journal of Mining Science and Technology · 2026
- Experimental study on dynamic mechanical properties and damage mechanisms models of concrete under freeze-thaw cyclesScientific Reports · 2026
- Study on the characteristics of concrete freeze-thaw cycling based on acoustic methodsConstruction and Building Materials · 2026