Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure Inclination
Haiquan Wang, Haofei Liu, Song Jiang, Zhao Wang, Min Yang, Lihai Tan, Tao Xue
Key points
From the paper's conclusion- Intact sandstone and parallel double-flawed sandstone with fissure inclinations of 30°, 45°, and 60° were therefore tested in uniaxial compression after 0, 10, 20, 30, and 50 freeze–thaw cycles, with digital image correlation (DIC), acoustic emission (AE), and scanning electron microscopy (SEM) linking macroscopic degradation to strain localization, crack activity, and microstructural change.
Abstract
Fissured rock masses in cold regions undergo matrix deterioration and structural weakening simultaneously, and separating the contribution of each remains difficult. Intact sandstone and parallel double-flawed sandstone with fissure inclinations of 30°, 45°, and 60° were therefore tested in uniaxial compression after 0, 10, 20, 30, and 50 freeze–thaw cycles, with digital image correlation (DIC), acoustic emission (AE), and scanning electron microscopy (SEM) linking macroscopic degradation to strain localization, crack activity, and microstructural change. Peak strength and apparent elastic modulus generally decreased with freeze–thaw cycling: after 50 cycles, the peak strength of intact specimens decreased from approximately 148 to 100 MPa, while the mean apparent elastic modulus of the 60° flawed group decreased from 13.14 to 6.49 GPa (49.36% retained). Freeze–thaw treatment altered the progressive development of surface strain localization and was associated with earlier AE activity, whereas fissure inclination influenced the spatial distribution of localized deformation and the resulting failure modes. Analysis based on the ratio of rise time to amplitude (RA) and average frequency (AF) showed a growing proportion of tensile cracking in every configuration; the 45° group shifted from 55.39% shear-dominated to 68.23% tensile-dominated. SEM images recorded progressive pore enlargement, interfacial debonding, and particle spalling. This study provides experimental evidence linking freeze–thaw-induced mechanical degradation with fissure inclination-dependent damage localization and fracture evolution in double-flawed sandstone. Freeze–thaw cycling thus sets the deterioration level of the material, while fissure inclination directs where and how failure develops.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanical behavior and multiscale damage evolution of filled fractured sandstone under freeze-thaw cycles.Scientific reports · 2026
- Progressive Asymmetry Damage Behavior and Macro–Micro-Scale Coupled Constitutive Modeling of Sandstone with Intersecting Fractures Under Freeze–Thaw Cycles and LoadingSymmetry · 2026
- Mechanical Response and Macro–Micro Damage Mechanisms of Sandstone Under Low‐Frequency Cyclic Disturbance After Freeze–Thaw CyclingFatigue & Fracture of Engineering Materials & Structures · 2026
- Mechanical deterioration of flawed rocks under freeze-thaw and cyclic loadingJournal of Rock Mechanics and Geotechnical Engineering · 2026
- Experimental Investigation of Sandstone Damage Evolution and Failure Mechanisms Under Freeze–Thaw CyclesApplied Sciences · 2026
- Strength Degradation of Sandstone Under Coupled Loading and Freeze-Thaw Cycles: Experimental Study and Discrete Element Numerical Simulation.Materials (Basel, Switzerland) · 2026