Effect of Rolling Reduction and Inhibitor on the Microstructure Evolution and Magnetic Properties of Strip-Cast Grain-Oriented Silicon Steel
Fuyao Yang, Chengyu Liu, Yu Han, Dingfang Ke, Yang Liu, Nuojin Wang, Yuanxiang Zhang, Fangfang Wu
Key points
From the paper's conclusion- By tailoring the rolling reduction and inhibitor, a high magnetic induction B8 of 1.94 T and a low iron loss P1.7/50 of 1.33 W/kg were achieved.
Abstract
Fe–3 wt.% Si grain-oriented silicon steel with high magnetic induction was fabricated based on a twin-roll strip-casting (TRSC) process. Systematic investigation of first-stage cold rolling reductions revealed that increasing reduction enhances fragmentation of the initial <100> solidification texture and promotes fine, homogeneous precipitates. A 60% reduction yielded optimal primary recrystallized microstructure dominated by fine grains, strong {111}<112> texture and high density of precipitates. Appropriate inhibitors present in suitable amounts and in a metastable state were a prerequisite for complete secondary recrystallization. A sole MnS inhibitor failed to provide adequate inhibition, allowing non-Goss grains to gain a size advantage early in secondary recrystallization. Strip with high content Al exhibited excessively strong inhibition, possibly associated with nitriding during high-temperature annealing, suppressing abnormal growth of both Goss and non-Goss grains. Precipitates near the migrating Goss grain boundaries were observed to coarsen preferentially, which is proposed to weaken local pinning and facilitate boundary migration. The intrinsic characteristic of a high proportion of special grain boundaries for Goss grains and appropriate inhibitors are crucial for achieving a well-developed secondary recrystallization of Goss texture. By tailoring the rolling reduction and inhibitor, a high magnetic induction B8 of 1.94 T and a low iron loss P1.7/50 of 1.33 W/kg were achieved.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Dislocation-Loop-Induced Secondary Recrystallization in Fe-3 wt.% Si: Y-Stabilized 〈100〉 Loops as Inhibitor Alternatives.Materials (Basel, Switzerland) · 2026
- Microstructural Origin of Magnetic Properties in Grain-Oriented Silicon Steel: Shear Band Angle Control of Intraband Lattice Rotation.Materials (Basel, Switzerland) · 2026
- The influence of heating rate on the secondary recrystallization behavior of low-temperature grain-oriented silicon steelMetallurgical Research & Technology · 2026
- Effects of cold rolling routes on microstructure, texture evolution, and magnetic anisotropy of ultra-thin non-oriented electrical steelJournal of Materials Research and Technology · 2025
- Texture Evolution of Fe–3.27 wt.% Si Nonoriented Electrical Steel During Deformation and Recrystallizationsteel research international · 2026
- Influence of Silicon Content and Strain Accumulation on Mean Flow-Stress Behavior and Microstructural Restoration of High-Silicon Electrical SteelsMetallurgical and Materials Transactions A · 2026