The influence of heating rate on the secondary recrystallization behavior of low-temperature grain-oriented silicon steel
Huimin Zhang, Sihui Wu, Chengyuan Zhang, Zhongwang Wu, Baozhi Liu, Hao Zhang, Yu Zhang, Yiwei Li,
Key points
From the paper's conclusion- The results demonstrate that at a heating rate of 15 °C/h, the onset temperature of secondary recrystallization is 1080 °C and the completion temperature is 1090 °C; at a heating rate of 10 °C/h, the onset temperature is 1070 °C and the completion temperature remains at 1090 °C.
Abstract
The high-temperature annealing treatment of grain-oriented silicon steel is a complex process, and the heating rate significantly influences the formation of the strong Goss texture. This study investigates the impact of the heating rate on the secondary recrystallization behavior of low-temperature grain-oriented silicon steel during the high-temperature annealing process. The microstructure, microtexture, and precipitated phases of the samples were characterized using an optical microscope, field emission scanning electron microscopy (SEM) combined with electron backscatter diffraction (EBSD), and energy dispersive spectroscopy (EDS). The magnetic properties of the finished plates were evaluated using a TD8735 single-chip permeameter designed for silicon steel measurement. The results demonstrate that at a heating rate of 15 °C/h, the onset temperature of secondary recrystallization is 1080 °C and the completion temperature is 1090 °C; at a heating rate of 10 °C/h, the onset temperature is 1070 °C and the completion temperature remains at 1090 °C. An increase in the heating rate delays the onset of secondary recrystallization, and narrows the temperature range for secondary recrystallization. Under both heating rates, the test steel exhibits superior performance at a heating rate of 10 °C/h. The core loss P 1.7/50 reaches 1.02 W/kg, and the magnetic induction intensity B 800 reaches 1.88 T, which meets the magnetic induction index requirements for high magnetic induction grain-oriented silicon steel. The texture evolution trends under both heating rates are similar. Observations of the texture changes at a heating rate of 10 °C/h reveal that textures such as {411}<148> and {111}<112> gradually transform into the Goss texture as the annealing temperature increases. The Zener factor of inhibitor particles decreases with increasing annealing temperature under different heating rates. When the annealing temperature reaches 1070 °C, the Zener factor at a heating rate of 10 °C/h is lower than that at 15 °C/h, indicating that secondary recrystallization commences earlier at a heating rate of 10 °C/h.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Annealing Temperature on Recrystallization Behavior of 0.25 mm Thin-Gauge Non-Oriented Electrical SteelMetals · 2026
- Effect of Rolling Reduction and Inhibitor on the Microstructure Evolution and Magnetic Properties of Strip-Cast Grain-Oriented Silicon SteelMaterials · 2026
- Influence of Silicon Content and Strain Accumulation on Mean Flow-Stress Behavior and Microstructural Restoration of High-Silicon Electrical SteelsMetallurgical and Materials Transactions A · 2026
- Texture Evolution of Fe–3.27 wt.% Si Nonoriented Electrical Steel During Deformation and Recrystallizationsteel research international · 2026
- Dislocation-Loop-Induced Secondary Recrystallization in Fe-3 wt.% Si: Y-Stabilized 〈100〉 Loops as Inhibitor Alternatives.Materials (Basel, Switzerland) · 2026
- Microstructural Origin of Magnetic Properties in Grain-Oriented Silicon Steel: Shear Band Angle Control of Intraband Lattice Rotation.Materials (Basel, Switzerland) · 2026