Artificial UV Weathering of Retrieved Poly(vinyl butyral) Interlayer from Laminated Glass Waste: Effects of Residual Additives and Restabilization with Phenolic Antioxidants.
Vasilis Nikitakos, Athanasios D Porfyris, Triantafyllia Alevizaki, Eleni Rakanta, Beatriz Yecora, Angelica Perez, Rudolf Pfaendner, Constantine D Papaspyrides,
Laboratory of Polymer Technology, School of Chemical Engineering, National Technical University of Athens, 15780 Athens, Greece. · Department of Materials Science & Engineering, School of Chemical Engineering, Zographou Campus, National Technical University of Athens, 15780 Athens, Greece.
Key points
From the paper's conclusion- The results showed that u-PVB exhibited pronounced photooxidative degradation, while re-PVB remained comparatively stable.
Abstract
Poly(vinyl butyral) (PVB) is widely used as an interlayer in laminated safety glass in automotive and construction applications. The increasing quantities of PVB arising from end-of-life laminated glass represent a waste stream with significant potential for recycling. This study investigates the durability of high-quality retrieved PVB (re-PVB) separated from laminated glass wastes and evaluates the effect of restabilization against UV aging. Neat unplasticized PVB (u-PVB) and re-PVB were subjected to artificial UV weathering (ISO 4892-3) for up to 1500 h and then characterized in terms of chemical structure, yellowness, melt flow behavior and molecular weight. The results showed that u-PVB exhibited pronounced photooxidative degradation, while re-PVB remained comparatively stable. UV-Vis spectroscopy revealed the presence of residual UV absorbers in re-PVB, indicating that the components of the initial stabilization system might remain functional after the end of its life. Unexpectedly, the restabilization of re-PVB with phenolic antioxidants (AOs) reduced its photooxidative stability, despite their established effectiveness against thermo-mechanical degradation in melt reprocessing. A possible antagonistic effect was suggested between the newly introduced AOs and the residual stabilization system. These findings highlight that re-PVB is a valuable waste, and restabilization should be carefully considered when designing its second service life.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Green-Synthesized Silver and Nickel Oxide Nanoparticles as Photostabilizers for PVC Films Under Accelerated UV Irradiation.Polymers · 2026
- Preparation of UV Aging‐Resistant SBS Polymer‐Modified Asphalt and Its Underlying Aging Resistance MechanismJournal of Applied Polymer Science · 2026
- Structural and Functional Stability of Strontium Aluminate-Based Luminescent Composites After 15 Years of Natural Weathering (Indoors and Outdoors).Polymers · 2026
- Release Characteristics of Bisphenol A from Weathered Polycarbonate: An Artificial Weathering StudyApplied Sciences · 2026
- Assessment of adhesion and durability of laminated safety glass made from end-of-life float glassGlass Structures & Engineering · 2026
- Antioxidant Potential of Waste Lignin Phenolics and Their Role in Thermo-Oxidative Stabilization of Polyurethane MaterialsMacromol—A Journal of Macromolecular Research · 2026