Release Characteristics of Bisphenol A from Weathered Polycarbonate: An Artificial Weathering Study
Christian Piechotta, David del Agua, Mark Vreys, Sven Gestermann, Katrin Kalbfleisch
Key points
From the paper's conclusion- These results suggest that BPA releases from outdoor PC applications occur only during an initial weathering period and subsequently diminish to virtually zero.
Abstract
Bisphenol A (BPA) release from polycarbonate (PC) samples representative for major outdoor applications under environmentally relevant conditions has been characterized by a recently developed artificial accelerated weathering method. It simulates typical environmental stressors through controlled exposure to UVA radiation, rain, temperature, and humidity variations in a weathering chamber. The weathering chamber was modified to a closed-loop water cycle, enabling detection of potential accumulated BPA releases from the investigated samples at ultra-trace levels and excluding contamination. Four PC materials, representative of major outdoor applications, were investigated: (i) Reference PC with low UV absorber content, (ii) coextruded PC sheet with a high UV-absorber content surface layer, (iii) UV-cured coating protected PC for automotive headlamps, (iv) thermally cured polysiloxane hard-coated PC sheet. The artificial weathering tests resulted in consistently low accumulated BPA releases of at most 0.34 mg m−2 for samples with exposed PC surfaces. Samples with outer surfaces protected by commercial coatings revealed approximately two orders of magnitude lower releases, with cumulative BPA releases of 0.005 mg m−2 for the UV-cured coating-protected PC and 0.003 mg m−2 for the polysiloxane hard-coated PC. Across all cases examined, the release of BPA ceased after at most four to six weeks, corresponding to roughly 1–1.5 years of outdoor exposure in Central Europe if correlated based on applied UV radiation dose. Extended weathering for up to 11 weeks confirmed that no further BPA releases occurred after cessation. These results suggest that BPA releases from outdoor PC applications occur only during an initial weathering period and subsequently diminish to virtually zero. The observed release pattern can be plausibly explained by hydrolysis at the PC surface initially triggering minimal BPA releases, while progressive photo-degradation transforms the chemical composition in the topmost surface layer, which is hypothesized to cause the observed cessation of BPA releases.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Structural and Functional Stability of Strontium Aluminate-Based Luminescent Composites After 15 Years of Natural Weathering (Indoors and Outdoors).Polymers · 2026
- Combining suspect screening and advanced flow analysis for the investigation of UV-light exposed microplastics: Automatic dynamic bioaccessibility tests of plasticizers and degradation products.Talanta · 2026
- Autofluorescence-Free Sensing of Released Bisphenol A from Packaging Materials by a Persistent Luminescence AptasensorAnalytical Chemistry · 2025
- Artificial UV Weathering of Retrieved Poly(vinyl butyral) Interlayer from Laminated Glass Waste: Effects of Residual Additives and Restabilization with Phenolic Antioxidants.Materials (Basel, Switzerland) · 2026
- In Vitro Exposure Assessment Improves Hazard Ranking of Bisphenol A AlternativesChemical Research in Toxicology · 2026
- An IL/c-MWCNTs@Cu-ZIF-67-Modified Electrochemical Sensor for the Individual Determination of Bisphenol A and Bisphenol S in Plastic LeachatesChemosensors · 2026