Comparative Evaluation of Oscillating Fiber Laser Welding and GMAW/MAG for SAE 1010 Agricultural Wheel Rims.
Willian Queiroz, Francisco Briones, Carola Martínez, William Haupt
Postgraduate Program in Design and Manufacturing Processes (PPGPPF), Department of Mechanical Engineering, University of Passo Fundo (UPF), Br 285 km 292, Passo Fundo 99052-900, Brazil. · Escuela de Ingeniería Mecánica, Pontificia Universidad Católica de Valparaíso, Av. Los Carrera 01567, Quilpué 2430000, Chile.
Key points
From the paper's conclusion- This study evaluates oscillating fiber laser welding as an alternative to gas metal arc welding with an active shielding gas (GMAW/MAG) for manufacturing 4.25 mm thick SAE 1010 agricultural wheel rims.
Abstract
This study evaluates oscillating fiber laser welding as an alternative to gas metal arc welding with an active shielding gas (GMAW/MAG) for manufacturing 4.25 mm thick SAE 1010 agricultural wheel rims. A systematic product development approach guided technology selection. The comparison included process energy, weld geometry, microstructure, grain size, Vickers microhardness, guided-bend testing, and industrial forming. Estimated GMAW/MAG heat input was 0.64 kJ/mm, whereas nominal incident laser energy was 0.019 kJ/mm; these quantities do not represent equivalent measurements of absorbed heat. Measurements from one transverse cross-section per welding condition showed a smaller weld-face width (5.70 vs. 12.97 mm), lower convexity (0.56 versus 3.93 mm), and a narrower heat-affected zone (0.85 versus 2.10 mm) for laser welding compared with GMAW/MAG. Less grain coarsening was observed in the laser-welded heat-affected zone. Mean fusion-zone hardness was 158.6 ± 18.9 HV1 for laser welding and 190.4 ± 11.0 HV1 for GMAW/MAG. Both conditions passed the guided-bend tests. All ten laser-welded specimens completed industrial forming, whereas two of ten GMAW/MAG specimens fractured during cone opening. The examined laser-welded cross-section exhibited a narrower weld profile than the examined GMAW/MAG cross-section. The laser-welding manufacturing route also eliminated the post-weld grinding operation under the investigated conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Welding Speed on the Properties of Laser Beam Welded 3 mm Thick Ti-6Al-4V Butt JointsAdvances in Materials Science · 2026
- Factorial Experiments on Laser Pre‐Treatment of Low‐Carbon Steel Welds Prior to the Application of Organic CoatingsMaterials and Corrosion · 2026
- Effect of oscillating arc motion in pulsed arc GMAW-WAAM: a multi-aspect study of additively manufactured AM70 high-strength low-alloy steelJournal of Adhesion Science and Technology · 2025
- An investigation of the effect of GMAW and SMAW processes on mechanical and microstructural properties of welded E350 grade steelScientific Reports · 2025
- Comparison of the Mechanical Behavior of AA5052 and AA6261 Dissimilar Joints by Friction- Stir Welding and Gas Metal Arc WeldingMetals · 2026
- Joining of Al 5052 Alloy to Advanced High-Strength Steel Sheets of Dissimilar Thickness Using Laser-Assisted Friction Stir Welding.Materials (Basel, Switzerland) · 2026