From the paper's conclusion- A full factorial design was applied to low‐carbon steel welds with imperfections and varying preparation methods (blast‐cleaning, mechanical grinding, laser‐based treatments).
Abstract
Effects of weld treatment methods on the performance of organic coatings during accelerated offshore cycle tests were statistically investigated. A full factorial design was applied to low‐carbon steel welds with imperfections and varying preparation methods (blast‐cleaning, mechanical grinding, laser‐based treatments). Laser treatment was evaluated as a supplementary method and as a stand‐alone approach. Surface preparation was the dominant investigated main factor influencing coating damage, with additional significant contributions from weld position, imperfection type, and exposure time. Preparation methods combining laser treatment with mechanical treatment performed equivalent to blast‐cleaning. Purely laser‐based methods, however, resulted in significantly higher damage levels. A key limitation of the 100 W ns‐pulsed laser process was the incomplete removal of silicate welding slag, leading to partial remelting and redeposition of glassy residues within weld grooves. The damage accumulation followed a two‐parameter Weibull model. Laser‐assisted weld preparation had the potential as an alternative to blast‐cleaning, provided that weld geometry is properly conditioned and laser parameters are appropriately scaled.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Laserbasierte lokale Oberflächenvorbereitung korrodierter Stahlbauteile: vom Prozessfenster zur FeldvalidierungStahlbau · 2026
- Effect of multilayer laser cladding on the microstructure and wear resistance of SiC/Ni60A coatingsScientific Reports · 2026
- Nanosecond Laser Cleaning of 10CrNi2Mo3Cu2V Steel: Surface Cleaning, Oxidation Control and Welding Performance.Materials (Basel, Switzerland) · 2026
- Effect of Laser Remelting on the Microstructure, Mechanical and Tribological Properties of Detonation-Sprayed NiCrFeBSiC Coatings for Mechanical Engineering ApplicationsJournal of Manufacturing and Materials Processing · 2026
- Investigation of laser-flux cored arc hybrid welding of Q690D high strength steel: weld formation, microstructure evolution and mechanical performanceJournal of Materials Research and Technology · 2025
- Effect of Laser Post-Treatment on the Microstructure, Mechanical and Tribological Properties of Detonation- and Flame-Sprayed Ni–Cr–Fe–Si–B–C CoatingsCoatings · 2026