Effect of Vacuum Annealing Temperature on Optoelectrical Performance of IGZTO Films and Thin-Film Transistors.
Weicheng Cao, Liang Fang, Xia Zhao, Guoqing Zhang, Gaobin Liu, Fang Wu, Dan Liu, Wensi Cai,
Chongqing Key Laboratory of Interface Physics in Energy Conversion, College of Physics, Chongqing University, Chongqing 400044, China. · Key Laboratory of Optoelectronic Technology & Systems (Ministry of Education), College of Optoelectronic Engineering, Chongqing University, Chongqing 400044, China.
Key points
From the paper's conclusion- The carrier concentrations and Hall mobilities of IGZTO films vary with the annealing temperature in the range of 7.44 × 1018 ~ 6.37 × 1019 cm−3 and 20.89~35.53 cm2·V−1·s−1, respectively.
Abstract
Thin-film transistors (TFTs) based on quinary indium-gallium-zinc-tin oxide (IGZTO) were fabricated via radio frequency (RF) magnetron sputtering. The impact of vacuum annealing temperatures (25-450 °C) on the microstructural and optoelectrical properties of films and TFTs was systematically investigated. All IGZTO thin films are amorphous and transparent, with optical bandgaps ranging from 3.22 eV to 3.63 eV. The one annealed at 350 °C exhibited the smoothest surface. The carrier concentrations and Hall mobilities of IGZTO films vary with the annealing temperature in the range of 7.44 × 1018 ~ 6.37 × 1019 cm-3 and 20.89~35.53 cm2·V-1·s-1, respectively. Oxygen vacancies (VO×) are considered the major origin of the conductivity of IGZTO films, and their evolution with annealing temperatures was elucidated. The TFT annealed at 350 °C achieved a saturation mobility (μsat) of 19.7 cm2 V-1 s-1, threshold voltage (VTH) of 4.72 V, subthreshold swing (SS) of 0.56 V dec-1, and Ion/Ioff of 8.1 × 107, but TFTs annealed at other temperatures show no switching behaviour. TCAD simulations indicate that vacuum annealing elevates VO× density, especially at the film surface; the switching failure at 150 °C and 450 °C is attributed to the pronounced structural disorder expressed by large characteristic slope energies of tail states, while the failure at 250 °C is due to excessive VO× density. This work may provide useful guidance for the performance optimisation of IGZTO film and TFTs via annealing.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Annealing-Temperature-Dependent Electrical and Optical Performance of Solution-Processed Amorphous IGZO TFTsTechnologies · 2026
- Air-annealing-induced vertical elemental gradients regulate defect chemistry and optoelectronic properties of cylindrical-target-sputtered ITO thin films.RSC advances · 2026
- Effects of Ga and Si Incorporation on Oxygen-Related Defects and Bias-Temperature Stability of ZnSnO Thin-Film Transistors.Micromachines · 2026
- Optimization of RF Sputtering Power for High-Performance ITZO Thin-Film Transistors: Correlation Between Film Properties, Oxygen Defects and Electrical PerformanceInorganics · 2026
- Amorphous IGZO Thin‐film Transistors: Materials, Device Structures, Fabrications, and Application ExplorationsAdvanced Functional Materials · 2025
- High-Performance Self-Aligned InGaZnO Thin-Film Transistor with Boron Ion Implantation into Source/Drain RegionsACS Applied Electronic Materials · 2026