Xikai Zhou, Hongliang Xiang, Qinchang Wu, Jiawei Liu, Xiaoqiang Cai, Gang Mu, Yang Li, Chaochao Wu
School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350108, China. · School of Advanced Manufacturing, Fuzhou University, Jinjiang 362251, China.
Key points
From the paper's conclusion- However, the interaction between oxygen-modified Marangoni convection and evaporation-induced recoil pressure during laser powder bed fusion (LPBF) remains insufficiently understood.
Abstract
Ti-15Zr alloys offer favorable biocompatibility, and interstitial oxygen provides an attractive pathway for further strengthening. However, the interaction between oxygen-modified Marangoni convection and evaporation-induced recoil pressure during laser powder bed fusion (LPBF) remains insufficiently understood. A three-dimensional multiphysics thermal-fluid model incorporating recoil pressure and temperature- and oxygen-dependent surface tension was developed. Surface-tension-only, recoil-pressure-only, and coupled simulations were compared on an idealized solid substrate, followed by discrete powder-bed simulations. Increasing oxygen content shifts the dominant Marangoni flow from outward spreading to inward convergence. Recoil pressure primarily drives central depression, whereas Marangoni convection redistributes molten metal. In transverse sections, low-oxygen outward flow competes with recoil-driven downward transport and promotes lateral spreading, whereas high-oxygen inward flow reinforces downward circulation. In longitudinal sections, reversed Marangoni flow suppresses recoil-driven rearward transport and promotes recirculation behind the vapor depression. Increasing oxygen content from 0 to 1.0 wt.% raises the top-view projected-area fraction with dσ/dT > 0 from 41.8% to 63.0%. Under powder-bed conditions, the mean track width in the central region decreases from 61.32 to 51.23 μm (16.5%), while the mean depth increases from 47.71 to 49.95 μm (4.7%). The findings provide a physical basis for regulating melt pool evolution in LPBF Ti-15Zr alloys.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- In-situ observation and simulation of melt pool evolution and single-track formation in laser claddingJournal of Materials Research and Technology · 2025
- Effects of Laser Process Parameters on Melt Pool Thermodynamics, Surface Morphology and Residual Stress of Laser Powder Bed-Fused TiAl-Based CompositesMetals · 2025
- The influence of laser power modulation on melt pool dynamics in laser powder bed fusionJournal of Applied Physics · 2025
- On Porosity Analysis of Ti-6Al-4V Thin Struts Made by Laser Powder-Bed Fusion: Effects of Build Orientation, Strut Size and Linear Energy DensityJournal of Manufacturing and Materials Processing · 2026
- Multiscale evolution of TiC particles in GH3536-based composites fabricated via laser powder bed fusion: coarsening mechanisms and hierarchical distributionInternational Journal of Extreme Manufacturing · 2026
- Fitting-Free Diagnosis of Conduction-Model Breakdown in Laser Powder Bed Fusion.Materials (Basel, Switzerland) · 2026