Abstract

Large-scale irregular cracks developed on the second-floor roof slabs of an industrial plant shortly after formwork removal. To identify the cracking mechanism and optimize the strengthening scheme, field inspection, X-ray diffraction (XRD) phase analysis, restrained-shrinkage stress calculation, and nonlinear finite element (FE) simulation were combined in a closed-loop study. The concrete strength, reinforcement arrangement, slab thickness, and flexural capacity all met the specification requirements, and XRD detected no crystalline sulfate-bearing phases within the 1-2 wt.% detection limit, ruling out structural overloading and sulfate-type chemical attack. The cracking was attributed mainly to excessive restrained drying-shrinkage stress caused by mix-proportion defects (a high water-to-binder ratio, excessive fly ash, and a high mud content in the fine aggregate); the calculated maximum restrained shrinkage stress of 3.19 MPa exceeded the concrete tensile strength. Preferential microcrack initiation in the aggregate-mortar interfacial transition zone (ITZ) is presented as a proposed mesoscale mechanism, because direct microstructural (SEM) observation was not performed. Under identical total CFRP consumption, a four-dimensional evaluation (bearing capacity, material utilization, crack suppression, and relative interfacial slip) showed that the grid-shaped layout outperformed the cross- and hash-shaped layouts, and a ±10% sensitivity analysis kept all predicted crack-width variations within ±5%. A composite remediation of low-pressure grouting plus grid-shaped CFRP was then applied; after 12 months of monitoring, the maximum crack width decreased from 0.32 to 0.04 mm, demonstrating the synergistic effect of the composite system rather than CFRP alone. This case provides a reference for the diagnosis and treatment of shrinkage cracking in comparable industrial roof slabs.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers