From the paper's conclusion- Spectral compatibility should therefore be verified rather than presumed.
Abstract
Polymerization of resin-based composites depends on an overlap between photoinitiator absorption and light-curing unit (LCU) emission, yet resins that fail to cure cannot be measured and go unreported. This study tested how photoinitiator chemistry and concentration interact with light-emitting diode (LED) emission spectrum, documenting outcomes photographically. Sixteen unfilled bisphenol A glycerolate dimethacrylate/triethylene glycol dimethacrylate (Bis-GMA/TEGDMA; 1:1 wt/wt premixed resin blend) formulations containing camphorquinone (CQ) combined with ethyl 4-(dimethylamino)benzoate (EDAB), 1-phenyl-1,2-propanedione (PPD), diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide (TPO), or phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide (BAPO) at four concentrations were cured for 20 s with a single-emission-peak (SLED) or multiple-emission-peak (MLED) LED unit (n = 3; 96 specimens). Specimens were photographed and classified as fully polymerized, partially polymerized, or unpolymerized; degree of conversion (DC) was measured by attenuated total reflectance Fourier-transform infrared spectroscopy (ATR-FTIR) and analyzed by two-way analysis of variance (ANOVA) and Tukey's honestly significant difference (HSD) tests (α = 0.05). Formulation, LCU, and their interaction significantly affected DC (p < 0.001), and these effects remained significant when specimens assigned 0% DC were excluded. CQ+EDAB was the only system that polymerized fully with both units (58.6-76.5%). CQ+TPO achieved a maximum DC of 68.5% with the MLED, which was not statistically significantly different from the highest value obtained with CQ+EDAB. However, when polymerized with the SLED, CQ+TPO produced unpolymerized specimens that could not be measured at any of the tested concentrations. CQ+BAPO responded to both units, more strongly to the MLED (61.2% vs. 48.1%). CQ+PPD, formulated without an amine co-initiator, failed with both units (≤6.7%). Photographic classification agreed with ATR-FTIR and recorded the outcome where spectroscopy was impossible. Higher radiant exposure outside the photoinitiator absorption band did not compensate for spectral mismatch, whereas within the band, conversion also depended on irradiance and photoinitiator concentration. Spectral compatibility should therefore be verified rather than presumed.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Photoinitiator Systems in Dental Resin-Based Composites: Mechanisms, Performance, and Clinical ImplicationsF1000Research · 2026
- Spatio-temporal optical and thermal monitoring reveals light-source- and photoinitiator-dependent cure heterogeneity in experimental resin-based composites.Dental materials : official publication of the Academy of Dental Materials · 2026
- Blue‐Light Activated Anthraimidazol‐Dione Photoinitiators for Efficient Free‐Radical Polymerization in the Context of Dental Material ApplicationsJournal of Applied Polymer Science · 2026
- Influence of Light-Curing Parameters on the Physicomechanical and Polymerization Properties of Bulk-Fill Resin Composites: A Scoping ReviewDentistry Journal · 2026
- Effect of Light-Curing Distance on Polymerization Behavior of Resin Composites: A Systematic Review and Meta-AnalysisPhyschem · 2026
- Quinoline-based Photoinitiators for Vat Photopolymerization: Synthesis and Formulation Design for 3D Printing.ACS polymers Au · 2026