Interfacial Microstructure and Tensile-Shear Properties of AA1060/SUS304 Dissimilar Sheet Joints Fabricated by Uniform-Pressure Electromagnetic Pulse Welding.
Zhisong Fan, Ying Huang, Shu Zhang, Jianghua Deng, Hanwei Ning, Minjie Huang
School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350116, China.
Key points
From the paper's conclusion- The results showed that straight interfaces without a transition zone exhibited hardness values between those of the base materials, whereas wavy interfaces with a transition zone showed higher hardness values than both parent materials.
Abstract
Compared with single-turn coil magnetic pulse welding, magnetic pulse welding using a uniform-pressure electromagnetic actuator (UP-EMPW) can provide a larger area of uniform pressure and address issues such as low energy utilization efficiency and short coil lifespan. In this work, AA1060 aluminum sheets were joined to SUS304 stainless steel sheets by UP-EMPW. The effects of discharge voltage and initial gap on the interfacial microstructure and mechanical properties of the joints were investigated by optical microscopy, scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), and tensile shear tests. Two distinct interface morphologies were observed: wavy interfaces and straight interfaces. Their formation was influenced by the combined effects of discharge voltage and initial gap. Microhardness measurements across the weld interface were further conducted to evaluate the local mechanical response and to help interpret the strengthening mechanisms associated with different interfacial features. The results showed that straight interfaces without a transition zone exhibited hardness values between those of the base materials, whereas wavy interfaces with a transition zone showed higher hardness values than both parent materials. Although these hardness data should be considered qualitative because of the limited indentation spacing, the overall trend suggests a stronger local strengthening effect at the wavy interface. The tensile shear tests indicated that the maximum load first increased and then decreased with increasing discharge voltage or initial gap. The highest joint performance within the investigated range was obtained at a discharge voltage of 9 kV and an initial gap of 1.5 mm, with a mean maximum tensile-shear load of 3288 ± 256 N and failure in the aluminum base material. The improved mechanical performance appeared to result from the combined effects of mechanical interlocking and metallurgical bonding associated with the wavy interface and transition zone. Fracture surface analysis further showed that base material fractures exhibited mixed ductile and brittle features, whereas pull-out failures were characterized by localized bonding and limited interfacial bonding.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructural Evolution and Mechanical Properties of AA2017 Aluminum Alloy Joints Produced by Rotary Friction Welding and TIG Welding.Materials (Basel, Switzerland) · 2026
- Microstructure and properties of rotating magnetic field-assisted laser welded 304 stainless steel jointsJournal of Materials Research and Technology · 2025
- Effect of tool geometry and welding parameters on shear strength and microstructural characteristics of AA6061-T6/PMMA friction stir lap jointsAdvances in Science and Technology – Research Journal · 2026
- Metallurgical and Mechanical Property Investigation of ETP Cu Similar Hybrid Friction Welds for Nuclear Fusion Applications.Materials (Basel, Switzerland) · 2026
- Microstructural Evolution and Mechanical Weakening Mechanisms in Pulsed Laser Powder‐Fed Welding of Dissimilar AA2195‐T8/AA7075‐T6 Aluminum Alloy JointsAdvanced Engineering Materials · 2026
- Effect of oscillating arc motion in pulsed arc GMAW-WAAM: a multi-aspect study of additively manufactured AM70 high-strength low-alloy steelJournal of Adhesion Science and Technology · 2025