Experimental Study on the Bearing Capacity of Fiber-Reinforced Geopolymer Pipes.
Shukang Ying, Lin Hu, Fang Xu, Peng Zhang, Wendong Fan, Wei Luo, Shichong Yang
Department of Underground Space, School of Engineering, China University of Geosciences (Wuhan), Wuhan 430074, China. · Hubei Wujing Freeway Development Co., Ltd., Wuhan 430010, China.
Key points
From the paper's conclusion- The results show that the unreinforced pipes exhibited brittle failure with four-lobe cracking.
Abstract
To investigate the mechanical behavior and failure mechanisms of fiber-reinforced geopolymer drainage pipes under three-edge bearing loads, three-edge bearing tests were conducted on unreinforced engineered geopolymer composite (EGC) and polyvinyl alcohol fiber-reinforced engineered geopolymer composite (PVA-EGC) pipes, as well as glass fiber-reinforced polymer (GFRP)-reinforced EGC and PVA-EGC pipes. The effects of different matrix materials and reinforcement types on the bearing capacity, crack development, and strain field evolution were systematically analyzed based on the load-displacement response, crack evolution, and distributed fiber optic monitoring. The results show that the unreinforced pipes exhibited brittle failure with four-lobe cracking. The bridging effect of PVA fibers delayed crack propagation and improved the post-cracking bearing capacity and structural integrity. The ultimate bearing capacity increased from 2489.38 N for the EGC pipe to 3088.98 N for the PVA-EGC pipe, representing an increase of 24.1%. For the reinforced pipes, the cracking load increased from 7215.18 N for the GFRP-reinforced EGC pipe to 15,339.56 N for the GFRP-reinforced PVA-EGC pipe, corresponding to an increase of 112.6%. The ultimate bearing capacity increased from 18,123.94 N to 24,855.69 N, representing an increase of 37.1%. The GFRP-reinforced PVA-EGC pipe exhibited a more gradual decrease in post-peak bearing capacity and improved deformation resistance and structural ductility. Crack analysis showed that PVA fibers effectively restrained crack localization. The cracking mode changed from through-cracks to multiple fine and uniformly distributed cracks, significantly improving the crack control capacity of the pipe. In addition, the combined action of PVA fibers and GFRP reinforcement reduced strain concentration and promoted more uniform stress transfer. This delayed crack propagation and the development of the GFRP reinforcement toward its ultimate stress state, thereby improving the overall bearing performance of the pipe.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of fibers on the multiscale properties of fly ash and slag based geopolymer foam concreteConstruction and Building Materials · 2026
- Dynamic Compressive Behavior and Internal Damage Evolution of Polypropylene Fiber-Reinforced Alkali-Activated Slag Geopolymer Mortar.Materials (Basel, Switzerland) · 2026
- Influence of hybrid fiber content on the mechanical performance of geopolymer compositeIOP Conference Series: Earth and Environmental Science · 2026
- Effect of Glass Fibers and Recycled Concrete Aggregates on the Properties of Geopolymer ConcreteBuildings · 2026
- Comparative Performance of Polyethylene- and Carbon Fiber-Reinforced Slag/Fly Ash Blended Geopolymer ConcreteBuildings · 2026
- Bond failure of corroded rebar embedded in rubberized geopolymer concrete: Experimental evaluationConstruction and Building Materials · 2026