Dynamic Compressive Behavior and Internal Damage Evolution of Polypropylene Fiber-Reinforced Alkali-Activated Slag Geopolymer Mortar.
Binghui Cui, Yanzhu Liu, Liang Wang
School of Management Engineering, Qingdao University of Technology, Qingdao 266500, China. · Engineering Research Center , Ministry of Education for Underground Mining Engineering, Anhui University of Science and Technology, Huainan 232001, China.
Key points
From the paper's conclusion- These results indicate that, within the tested range, a PPF content of 1.0% is effective for impact-resistant geopolymer mortar.
Abstract
Ordinary Portland cement (OPC) production is energy- and carbon-intensive, which has motivated the development of more sustainable alternatives such as alkali-activated materials, including granulated blast furnace slag (GBFS) geopolymer mortar. Geopolymer mortar, however, is brittle, has low tensile strength and poor crack resistance, and its damage evolution under dynamic impact remains insufficiently understood. Here we show that polypropylene fiber (PPF) reinforcement substantially improves the dynamic impact resistance of GBFS-based geopolymer mortar with only a limited effect on static compressive strength. Mortars with PPF volume contents of 0%, 0.2%, 0.4%, 0.6%, 0.8%, and 1.0% were prepared at a water-to-binder ratio of 0.55. Flowability, static compressive strength, and dynamic mechanical properties were evaluated using a split Hopkinson pressure bar at strain rates of 50 s-1-130 s-1, and failure morphology was examined through SEM and CT analysis. Increasing PPF content reduced flowability from 253 mm to 224 mm at 1.0% but had little effect on static strength. Dynamic compressive strength, dynamic increase factor (DIF), and ultimate toughness increased with both strain rate and fiber content. The 1.0% PPF mortar reached a maximum DIF of 2.129 and a 99.3% increase in impact toughness. CT analysis further showed that PPF suppressed the formation of large internal voids: approximately 31, 2, and 5 voids larger than 4 mm3 were detected in the 0.6%, 0.8%, and 1.0% PPF specimens, respectively. The improvement is attributed to fiber bridging and pull-out, which consume impact energy and inhibit crack initiation and propagation. These results indicate that, within the tested range, a PPF content of 1.0% is effective for impact-resistant geopolymer mortar.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Combined Effects of Foundry Sand Replacement and Polypropylene Fiber Content on Slag Geopolymer Mortar PropertiesBuildings · 2026
- High-Performance Self-Stratifying Fiber-Reinforced Mortar for Airport Pavement Thin-Layer Repair: OPC-SAC Hybrid System OptimizationBuildings · 2026
- Influence of Steel and Polypropylene Fibers on Flexural Strength and Fracture Properties of Ambient-Cured Geopolymer ConcretePolymers · 2026
- Influence of fibers on the multiscale properties of fly ash and slag based geopolymer foam concreteConstruction and Building Materials · 2026
- Effect of Copper Slag Content and Hybrid Steel Fiber Addition on the Mechanical Response of an Alkali-Activated Geopolymer CompositeFibers · 2026
- Residual Mechanical Performance and Mass Loss of Heat-Cured NaOH-Activated Fly Ash/Slag and Portland Cement Mortars After Exposure to Elevated TemperaturesBuildings · 2026