Compression-Shear Hysteretic Performance of Circular Section Members Strengthened with CFRP-Wrapped Steel Tube Confined Concrete.
Kuan Peng, Qingli Wang, Libo Wan
School of Mechanical Engineering, Chengdu Technological University, Chengdu 610031, China. · School of Civil Engineering, University of Science and Technology Liaoning, Anshan 114051, China.
Key points
From the paper's conclusion- The results indicate that the specimens exhibit a stable four-stage mechanical response and typical failure modes, including steel tube shear fracture, CFRP tensile fracture, and concrete shear fracture.
Abstract
A multi-faceted research framework integrating experimental tests, finite element (FE) simulations, and parametric analysis was adopted to investigate the compression-shear hysteretic performance of CFRP-confined concrete-filled steel tubes (CFRP-CFST). Nine circular specimens were designed, with the axial compression ratio and transverse CFRP confinement coefficient as key variables, to conduct material performance tests, laying a foundation for subsequent research. Displacement-controlled cyclic loading was applied in the tests to obtain hysteretic curves, observe the failure process, and calculate stiffness degradation and strength degradation. FE models were established using the constitutive relationships of corresponding materials and material parameters derived from tests (e.g., concrete plastic damage coefficients), and their reliability was verified by comparing simulation results with experimental data. Further stress analysis throughout the loading process was performed to reveal the stress distribution and evolution laws of concrete, steel tubes, and CFRP during loading. Finally, parametric analysis was carried out to explore the effects of material strength, transverse CFRP layers, and axial compression ratio on the hysteretic performance of the members. The results indicate that the specimens exhibit a stable four-stage mechanical response and typical failure modes, including steel tube shear fracture, CFRP tensile fracture, and concrete shear fracture. The established FE models can reliably predict the hysteretic characteristics and failure mechanisms of the specimens. While material strength, CFRP layers, and axial compression ratio significantly enhance the peak bearing capacity, they have little impact on the initial elastic stiffness or the overall trend of the skeleton curve. In addition, the steel tube and CFRP maintain effective synergy, improving the ductility and energy dissipation capacity of the members.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Behavior of FRP‐Reinforced Concrete Columns Subjected to Combined Axial Compression and Lateral LoadingAdvances in Civil Engineering · 2026
- Axial Compressive Behaviour of Intermediate-Length Concrete-Filled Steel Tubular Columns with Different CFRP Wrapping ConfigurationsBuildings · 2026
- Seismic performance of externally stiffened ring connections between concrete-filled steel tubular columns and reinforced concrete beamsScientific Reports · 2026
- Experimental and numerical investigations of UHPFRC-filled circular steel tubular columns under axial and lateral cyclic loadsScientific Reports · 2026
- Parametric Study on Seismic Performance of FRP-RC Exterior Beam-Column Joints.Polymers · 2026
- Compression–bending resistance of corrugated steel tube‐confined rubberized concrete columns considering non‐uniform confinementStructural Concrete · 2026