Study on Preparation and Hydration Mechanism of Sand Washing Residue Mud-Based LC3 Cement by Mechanical-Thermal Activation.
Gang Wang, Keliang Li, Linhua Jiang, Junjie Ma, Yichuan Yan, Hengjun Hou, Huanqiang Liu, Weizhun Jin
China Construction Seventh Engineering Division Co., Ltd., Zhengzhou 450004, China. · School of Civil Engineering and Transportation, North China University of Water Resources and Electric Power, Zhengzhou 450045, China.
Key points
From the paper's conclusion- The results showed that within a ball-milling time range of 3-9 min, as the ball-milling time increased, the specific surface area increased, the median particle size D50 decreased, and the particle size was mainly concentrated within the range of 0.1-30 μm; the specific surface area of the washed sand residue after 3 min of grinding reached 1080 m2/kg, with D50 being 3.50 μm, which met the requir
Abstract
To enhance the application value of sand washing residue mud (SWRM) and mitigate its adverse environmental impacts, this study focuses on the resource utilization of SWRM. The research employed a combined mechanical-thermal activation method to enhance the activity of SWRM and utilized the mixed optimal design module to design and optimize the mixing ratio of SWRM-based LC3 cement. The results showed that within a ball-milling time range of 3-9 min, as the ball-milling time increased, the specific surface area increased, the median particle size D50 decreased, and the particle size was mainly concentrated within the range of 0.1-30 μm; the specific surface area of the washed sand residue after 3 min of grinding reached 1080 m2/kg, with D50 being 3.50 μm, which met the requirements for making cementitious materials. After thermal activation at temperatures ranging from 450 °C to 950 °C for the 3 min ground SWRM, the 28 d activity index showed a trend of increasing first and then decreasing with the increase in calcination temperature, and the 28 d activity index reached the maximum of 79.3% at a calcination temperature of 650 °C. The optimal mixing ratio of the AC70 group's SWRM-based LC3 cement obtained through the mixing design was: cement clinker 66.5%, desulfurized gypsum 3.5%, activated SWRM 15%, and limestone powder (LP) 15%. The 28 d compressive strength of the AC70 group's SWRM-based LC3 cement was 34.1 MPa, with initial setting and final setting times of 170 min and 240 min respectively, and the volume stability was qualified. The microscopic test results indicated that under the synergistic effect of alkali and salt, the silicate and aluminosilicate tetrahedral structures in the active sand-washed mud (ASWRM) decomposed, forming a C-(A)-S-H network structure, which was the main source of strength for the SWRM-based LC3 cement in the later stage. The ecological benefit calculation and analysis showed that compared with ordinary Portland cement of the same grade, the AC70 group's SWRM-based LC3 cement had a 27.6% reduction in implicit energy consumption, a 44.1% reduction in carbon emissions, and a 25% reduction in cost. This study provides an innovative approach for the high value-added resource utilization of SWRM.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Synergistic utilization of bauxite residue (red mud) and multiple solid wastes for low carbon precast concrete materials: Mechanical performance, mechanism and sustainability assessmentGreen Energy and Resources · 2026
- Research Progress on the Preparation and Performance of Recycled Mortars Using Solid Waste-Based Cementitious MaterialsCoatings · 2025
- Comparative Assessment of Calcined and Mechanically Activated Muscovite Clay as Supplementary Cementitious Materialce/papers · 2026
- Wet-Grinding Reactivation and Frost Resistance of Waste Sludge from a Concrete Mixing Plant: A Case Study of Large-Scale Mine Construction in the Xinjie Taigemiao Mining Area.Materials (Basel, Switzerland) · 2026
- Low‐Carbon Composite Cement Mortar Incorporating Local Raw Materials as SCMs: Performance and Life Cycle AnalysisJournal of the American Ceramic Society · 2026
- Effect of multi-source solid waste synergistic activation on strength evolution and micro-mechanism of dredged sludge stabilized with low-carbon curing agent.PloS one · 2026