Root-Inspired Bio-Interlocking Structure Design and Its Mechanism on Enhancing the Interfacial Bonding of NiTi/Ti6Al4V Fabricated by MM-LPBF.
Jingyu Xu, Honglei Ge, Zhenyu Niu, Jiakun Shi, Shuitao Zhou, Juzhao Chen, Xuehao Gao, Haida Chen,
Research Centre for Laser Extreme Manufacturing, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China. · National Defence Key Discipline Laboratory of Light Alloy Processing Science and Technology, Nanchang Hangkong University, Nanchang 330063, China.
Key points
From the paper's conclusion- The results show that the branching angle is the primary factor determining the performance.
Abstract
The dissimilar combination of NiTi shape memory alloy and Ti6Al4V titanium alloy offers superelasticity, biocompatibility and high specific strength, showing broad application prospects in aerospace and medical fields. However, when fabricating NiTi/Ti6Al4V composite components by multi-material laser powder bed fusion (MM-LPBF), brittle cracks or even complete delamination easily occur at the interface. In this paper, without relying on intermediate interlayer materials, we innovatively propose a root-inspired three-dimensional bio-interlocking interface structure. By means of macroscopic three-dimensional geometric interlocking, the crack propagation path and load transfer mode are forced to change. Using the branching angle (45°, 60°) and the structural size multiplier (1.2, 1.5) as variables, the influence of the bio-inspired geometric parameters on the interfacial forming quality, microstructure and mechanical properties was systematically investigated. The results show that the branching angle is the primary factor determining the performance. The 45° low-angle branched specimens exhibit overall brittle delamination along the flat metallurgical reaction interface under shear loading, with an average shear strength of only 17.47 MPa. In contrast, the 60° high-angle branched specimens, owing to their larger normal embedding depth, exhibit a failure mode transitioning to a mixed mode that includes crack deflection, branch shearing and plastic tearing of the Ti6Al4V matrix. Although TEM confirms that a continuous Ti2Ni brittle phase still exists at the interface, the optimised 60-1.5 structure increases the average shear strength to 128.37 MPa, which is more than six times higher than that of the 45-1.2 group (17.47 MPa). This "geometrical constraint toughening" strategy provides a new paradigm for the interfacial strengthening of dissimilar metals without relying on metallurgical modification.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Lattice‐Defect‐Coordinated Microstructural Continuity and Mechanical Compatibility in LPBF‐Fabricated CoCrNi/316L Bimetallic StructuresRare Metals · 2026
- Weldability Improvement of Additively Manufactured Nickel-Based Superalloy by Controlling W and Si Migration at Solidification Front.Materials (Basel, Switzerland) · 2026
- Review of the laser powder bed fusion of nitinol: Defect formation and predictionMaterials Today Advances · 2026
- Fatigue and fracture properties of Al2618 + TiB2-reinforced metal matrix composite produced by Laser-powder bed fusionInternational Journal of Fatigue · 2026
- Niti minimal surface porous scaffolds matching human bone characteristics: mechanical, permeability and osteogenic propertiesVirtual and Physical Prototyping · 2026
- Laser directed energy deposition of NiTi shape memory alloys with herringbone grain architectures for enhanced ductility and superelasticityMaterials & Design · 2025