Weldability Improvement of Additively Manufactured Nickel-Based Superalloy by Controlling W and Si Migration at Solidification Front.
Rui Ma, Xin Xi, Zhaoyang Lin, Wenrui Luo, Yanhao Hou, Wenjun Zhao, Zhifeng Shi, Xiaoguo Song,
Beijing Power Machinery Institute, Beijing 100074, China. · Academy of Aerospace Liquid Propulsion Technology, Xi'an 710100, China.
Key points
From the paper's conclusion- Thus, TCP phase and silicides were transformed into carbides, which successfully suppressed weld cracking, reducing the crack depth ratio from 0.70 ± 0.08 to zero.
Abstract
Nickel-based superalloy components prepared by laser powder bed fusion (LPBF) are increasingly being used in the hot ends of aeroengines, which still need to be laser-welded to realize the assembly connection of large closed structures. However, the unique microstructural characteristics of LPBFed parts render them more poorly weldable than casts and wroughts, especially in cracking-sensitive superalloys. In this study, cracking mechanisms were analyzed by performing laser deep fusion welding on an LPBFed Haynes 230 alloy. The key factors leading to weld cracking were strongly correlated with the low-melting-point TCP phases enriched with W, Si, Al, and silicides, both of which tended to be distributed in the boron(B)-rich region and exhibited poor coherence with the matrix. In addition, the flow behavior of the molten pool affected the solidification rate of the weld, resulting in large solidification shrinkage stresses in the cracking-sensitive zone (CZ) part of the weld. In order to minimize the development conditions of the cracking-sensitive phases, reducing the content of W (from 14.96 to 13.56 wt.%) and Si (from 0.47 to 0.25 wt.%) was chosen to alleviate the segregation of W, Si and C elements in the solid phase at the end of solidification. Thus, TCP phase and silicides were transformed into carbides, which successfully suppressed weld cracking, reducing the crack depth ratio from 0.70 ± 0.08 to zero. New insights into the weldability improvement and crack inhibition mechanism of laser-welded additively manufactured cracking-sensitive superalloys are provided, accelerating the rapid application of large assemblies.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructural evolution and strengthening mechanisms of gas tungsten arc welded nickel-based superalloy joints processed by laser powder bed fusion: Effects of welding direction and heat inputJournal of Materials Processing Technology · 2025
- Laser beam powder bed fusion nickel-based superalloys: microstructure, alloy tailoring and mechanical propertiesVirtual and Physical Prototyping · 2026
- Synergistic Effects of Carbon/Nitrogen Content and Laser Powder Bed Fusion Parameters on the Hot Cracking Behavior and Microstructural Evolution of a Ni–Co‐Based SuperalloyAdvanced Engineering Materials · 2026
- Advances in laser powder bed fusion of hard-to-weld superalloys: a comprehensive reviewMaterials & Design · 2025
- Mechanistic process–microstructure–cracking correlations in laser powder bed fusion of the Ni-based superalloy IN738Materials & Design · 2026
- Specific point energy as a design parameter in L-PBF processes for novel additive manufacturing of pure tungsten parts for nuclear fusion applicationsThe International Journal of Advanced Manufacturing Technology · 2026