Rapid Repair Epoxy Mortar Fully Replacing Natural Aggregate and Filler with Graded Iron Tailings: Performance and Reinforcement.
Anhua Xu, Jiming Xiao, Yuchang Duan, Huaxin Chen, Jincheng Yu, Fayun Lei, Dongliang Kuang
School of Water Resources and Civil Engineering, Qinghai Polytechnic University, Xining 810003, China. · Qinghai Provincial Traffic Control Construction Engineering Group Co., Ltd., Xining 810028, China.
Key points
From the paper's conclusion- Numerous studies have investigated the application of iron tailings as raw materials for cement concrete, while rare efforts have been devoted to developing epoxy pavement repair mortars where graded IT function simultaneously as fine aggregate and filler.
Abstract
Numerous studies have investigated the application of iron tailings as raw materials for cement concrete, while rare efforts have been devoted to developing epoxy pavement repair mortars where graded IT function simultaneously as fine aggregate and filler. This study prepared epoxy resin mortar for rapid repair of cement concrete pavement using graded iron tailings (IT) as fine aggregate and filler. All mixtures employed IT as fine aggregate, where the mass proportion of IT filler relative to the total IT mixture varied from 0% to 40%. The effects of IT filler content on workability, curing temperature, mechanical properties, volume stability, and bond strength were investigated, accompanied by microstructural analysis. Experimental results reveal that the incorporation of IT filler ameliorates the fresh workability and shortens the setting time of epoxy mortar, whereas the compressive strength, flexural strength and interfacial bond strength exhibit an initial ascending followed by a descending trend with the increasing IT filler fraction. The optimal IT filler content is determined to be 20%. For fresh-state performance, the modified mortar delivers a flowability of 176.8 mm (+29.7% relative to EM-0) and a setting time of 127 min. In terms of hardened mechanical and bonding properties, the 28-day compressive strength, 28-day flexural strength and 7-day flexural bond strength reach 113.2 MPa (+17.2%), 42.5 MPa (+34.0%) and 9.1 MPa (+75.0%), respectively, in comparison with the reference specimen EM-0. Microscopic characterizations deliver indirect evidence that appropriate IT filler may refine internal pore-size distribution, densify matrix microstructure and suppress crack propagation. The failure mode changed from pure interfacial debonding to cohesive failure in the cement substrate. This work provides a green scheme for resource utilization of iron tailings in high-performance pavement repair materials.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Iron Tailing Powder-Granulated Blast Furnace Slag Composite Admixtures on the Mechanical Properties and Resistance to Chloride Erosion of Cement MortarBuildings · 2026
- Development and characterization of sustainable mortar using industrial iron waste as an alternative to sand with Portland limestone cementNext Materials · 2026
- Recycling Iron Ore Tailings as Sand Replacement in Cement Mortar: Effects on Strength, Durability, and MicrostructureArabian Journal for Science and Engineering · 2026
- Sulfate-alkali balance and fiber-matrix interactions regulate the microstructure, mechanical behavior, and environmental impact of ultra-fine tailings mortar.Environmental research · 2026
- Mechanically Activated Iron Tailings as Filler for Asphalt Mastic: High-Temperature Performance and Fatigue ResistanceSustainability · 2026
- Fiber-Reinforced One-Part Geopolymer Mortars Incorporating Red Mud, Ceramic Powder, and MgO: Performance Under Different Curing Regimes and Curing-Based Environmental Assessment.Polymers · 2026