Effect of SiC Content on Microstructure and Mechanical Properties of CoCrFeNi High-Entropy Alloy Composites
Ning Li, Xinlong Hu, Chengbo Wu, Mengyuan Jiang, Hui Li, Jinlong Zhang, F. D. Dong
North Minzu University
Key points
From the paper's conclusion- In this work, to address the limitation of low strength and hardness of single-phase CoCrFeNi high-entropy alloy, SiC particles were introduced as a reinforcing phase to prepare CoCrFeNi matrix composites with SiC contents of 0 wt%, 1 wt%, 2.5 wt% and 5 wt% via spark plasma sintering (SPS).
Abstract
In this work, to address the limitation of low strength and hardness of single-phase CoCrFeNi high-entropy alloy, SiC particles were introduced as a reinforcing phase to prepare CoCrFeNi matrix composites with SiC contents of 0 wt%, 1 wt%, 2.5 wt% and 5 wt% via spark plasma sintering (SPS). It was preliminarily predicted that SiC particles would be uniformly distributed along grain boundaries of the CoCrFeNi matrix. During sintering, partial SiC decomposes at high-temperature, high-activity interfaces, regulating carbide precipitation and phase structural evolution, while residual undecomposed SiC remains at grain boundaries to pin boundaries and refine grains, thereby synergistically enhancing mechanical properties and wear resistance. Microstructural characterization reveals that all samples maintain a face-centered cubic (FCC) solid-solution matrix, and samples with non-zero SiC addition contain Cr7C3 carbides, which are mostly distributed at grain boundaries. With the increase in SiC content, mechanical performance is remarkably improved compared with the unreinforced CoCrFeNi matrix: the hardness rises from 198.8 HV to 321.7 HV, the yield strength is greatly enhanced from 242.5 MPa to 673.4 MPa, and the tensile strength increases from 557.9 MPa to 755.7 MPa. The improved yield strength originates synergistically from grain refinement, solid-solution strengthening, grain-boundary strengthening and dislocation strengthening. By clarifying the influence of microstructural defects on critical shear stress (τ0) and normal fracture stress (σ0), the intrinsic mechanism governing tensile mechanical performance and ductile–brittle fracture transition was revealed. This optimized CoCrFeNi/SiC composite exhibits excellent strength–hardness comprehensive performance, showing promising application potential for high-load, wear-resistant and structural service components under severe tribological and pressure conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of SiC particle size on microstructure evolution and tribological behavior of CoCrFeNiAl coatings prepared by laser claddingJournal of Materials Research and Technology · 2025
- Silicon‐Induced Microstructural Refinement and Its Influence on Tribological and Corrosion Behavior of CoCrFeMnNi High‐Entropy AlloysAdvanced Engineering Materials · 2026
- In Situ Crystallization‐Induced Coherent Interfaces for Simultaneous Toughening and Hardening of Reinforced Silicon Carbide NanoceramicNational Materials · 2026
- Semi-solid brazing via CoCrFeNiCux high-entropy alloy fillers: interfacial microstructure, mechanical properties, and joining mechanism of C/C-SiC composites and TZM alloyAdvanced Composites and Hybrid Materials · 2026
- Effect of Ball Milling Time on the Microstructure and Mechanical Properties of Al0.2CoCrFeNi-5%WC High-Entropy Alloy Matrix Composite Prepared by Spark Plasma SinteringCoatings · 2026
- Multicomponent Si‐Rich σ Phase Induced Deterioration of Ductility and Strain Hardening in a (CoCrNi) 9 Si Medium‐Entropy AlloyAdvanced Engineering Materials · 2026