Coatings

Effect of Ball Milling Time on the Microstructure and Mechanical Properties of Al0.2CoCrFeNi-5%WC High-Entropy Alloy Matrix Composite Prepared by Spark Plasma Sintering

Hui Liang, Ziwen Hong, Qian Liu, Hesirui Guo, Wenyue Gu, Jingzhuo Zhang, Jinxin Hou, Jingchang Sun,

Key points

From the paper's conclusion
  • Herein, Al0.2CoCrFeNi-5%WC composites consolidated by spark plasma sintering at 1000 °C are systematically investigated to elucidate the effect of ball milling time (2–40 h) on microstructure and mechanical performance.

Abstract

The room-temperature strength of Al0.2CoCrFeNi high-entropy alloy (HEA) is insufficient for load-bearing applications despite its excellent ductility. Herein, Al0.2CoCrFeNi-5%WC composites consolidated by spark plasma sintering at 1000 °C are systematically investigated to elucidate the effect of ball milling time (2–40 h) on microstructure and mechanical performance. All composites comprise an FCC matrix, residual WC, and in situ M6C/M23C6 carbides; prolonged milling progressively elevates the total carbide fraction from 10.0% to 13.6% through enhanced interfacial reactions. The mechanical response is non-monotonic: the 10 h-milled sample exhibits the optimal strength–ductility synergy (ultimate compressive strength 2211 MPa and fracture strain 48.4%), whereas excessive milling (40 h) raises yield strength (878 MPa) and hardness (489 HV) at the expense of ductility (29.9%). Quantitative strengthening analysis identifies grain-boundary refinement and dislocation strengthening as the dominant contributions, with a minor load-transfer contribution, while residual work hardening and interfacial carbide networks govern the strength-ductility trade-off at extended milling. This work provides a processing-structure-property guideline for designing high-performance WC-reinforced HEA composites.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers