Lubricants

CeO2-Modified Ni201 Laser-Clad Coatings: Wear Behavior and Alkaline Corrosion Response

Haohao Cui, Yong Huang, Yaoning Sun, Qingyu Meng, Yang Li

Key points

From the paper's conclusion
  • Cross-sectional SEM observations indicated relatively sparse and small visible pores in the 0.5 wt.% CeO2 coating, whereas pores were more frequently observed in the 1.0 and 1.5 wt.% coatings.

Abstract

Ni201–CeO2 composite coatings containing 0–1.5 wt.% CeO2 were fabricated on 304 stainless steel by coaxial powder-fed laser cladding to investigate the effects of low-level CeO2 addition on a compositionally simple Ni-rich coating system. CeO2 addition did not produce a clear change in the dominant Ni-rich FCC solid-solution phase or measured bulk coating hardness. The 0.5 wt.% CeO2 coating, prepared from ball-milled powder, exhibited the lowest full-test average coefficient of friction (0.5330) and a 74.6% reduction in wear volume relative to the unmilled CeO2-free reference. Worn-surface observations showed a relatively regular wear track with less pronounced plastic smearing and no crack network comparable to that observed in the CeO2-free coating. Cross-sectional SEM observations indicated relatively sparse and small visible pores in the 0.5 wt.% CeO2 coating, whereas pores were more frequently observed in the 1.0 and 1.5 wt.% coatings. Electrochemical measurements in 1 mol L−1 NaOH showed parameter-dependent differences in OCP, apparent icorr, and fitted Rct, without a consistent overall ranking.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers