physica status solidi (a)

Microstructure and Wear Properties of Ti4822 Coatings Prepared by Laser Cladding

Yu Wu, Yongkun Li, Da Shu, Wenrui Li, Lin Xi, Jingming Tang

Key points

From the paper's conclusion
  • The highest measured hardness (727.67 HV under a 1 kgf load), lowest reported friction coefficient (0.43), and minimum wear mass loss (1.4 mg) occurred for the coating prepared with 1.0 wt% Ce.

Abstract

Ti4822 (Ti‐48Al‐2Cr‐2Nb) alloys are of interest for lightweight, high‐temperature applications. In this study, Ti4822 coatings containing 0–2.5 wt% Ce were deposited on TC4 substrates by laser cladding. Their microstructure, hardness, and sliding‐wear behavior were investigated experimentally, with idealized first‐principles calculations used for qualitative comparison. XRD patterns indicated that γ‐TiAl and α 2 ‐Ti 3 Al were the dominant identified phases. The highest measured hardness (727.67 HV under a 1 kgf load), lowest reported friction coefficient (0.43), and minimum wear mass loss (1.4 mg) occurred for the coating prepared with 1.0 wt% Ce. The worn‐surface observations suggested contributions from abrasive and adhesive wear, while the possible roles of oxide‐containing debris remain interpretive. The experimental findings identify 1.0 wt% Ce as the most favorable addition among the compositions tested; the calculations do not establish a unique strengthening mechanism for these multiphase coatings.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Microstructure and Wear Properties of Ti4822 Coatings Prepared by Laser Cladding — Science Skim