Reinforcement Corrosion in Coral Aggregate Concrete: 20-Month In-Situ Comparison of Portland, Magnesium Phosphate, and Hybrid Fly Ash–Silica Fume Binders in the South China Sea
Yating Li, Dapeng Zhang, Huiling Zhang, Xibing Lin, Qinghua Li
Key points
From the paper's conclusion- This study reports a 20-month in-situ exposure campaign on a natural reef-flat platform in Zhanjiang Bay, in which HRB400 carbon steel and 316L stainless steel rebars were embedded in CAC prepared with Portland cement (PC), magnesium phosphate cement (MPC), and a hybrid fly ash–silica fume binder (HF) at a fixed water-to-binder ratio of 0.30.
Abstract
Reinforcement corrosion is a governing durability concern for coral aggregate concrete (CAC) structures in the South China Sea, yet long-term field evidence comparing alternative binder systems under natural marine exposure remains scarce. This study reports a 20-month in-situ exposure campaign on a natural reef-flat platform in Zhanjiang Bay, in which HRB400 carbon steel and 316L stainless steel rebars were embedded in CAC prepared with Portland cement (PC), magnesium phosphate cement (MPC), and a hybrid fly ash–silica fume binder (HF) at a fixed water-to-binder ratio of 0.30. Open-circuit potential was monitored over early (0–5 months), middle (5–12 months), and late (12–20 months) exposure windows, and potentiodynamic polarization was measured at three snapshot ages (month 5; months 12–14; months 19–20), complemented by rapid chloride migration testing, XRD, and SEM–EDS. The corrosion behavior of carbon steel was strongly binder-dependent. In the MPC matrix, carbon steel underwent severe early-stage activation (icorr = 7.92 µA/cm2, equivalent to 91.9 µm/y), which is attributed to the near-neutral pore solution of the portlandite-free K-struvite matrix; the corrosion rate subsequently decreased by more than four orders of magnitude, a trend consistent with a transition toward transport-limited kinetics rather than a restoration of passivity. The HF binder yielded the lowest chloride migration coefficient (0.171 × 10−12 m2/s) and sustained low corrosion rates of carbon steel, plausibly reflecting pozzolanic pore refinement and chloride binding. 316L stainless steel remained below the RILEM TC 154-EMC passivity threshold (0.1 µA/cm2) in all three binders. These results suggest that binder–reinforcement compatibility, rather than matrix density alone, governs the long-term corrosion performance of CAC in reef-flat environments.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Comparative study on mechanical and corrosion resistance properties of magnesium ammonium/potassium phosphate cement coatings under stress and marine environmentREVIEWS ON ADVANCED MATERIALS SCIENCE · 2026
- Corrosion of Embedded Carbon Steels, Carbonation and Chloride Diffusion in Low-Clinker Hybrid and LC3-50 Cements: A Critical Review.Materials (Basel, Switzerland) · 2026
- Investigation of the Long-Term Corrosion Behavior of Steel in Nano-SiO2 Seawater ConcreteCoatings · 2026
- Properties of Eco-Friendly Grade C60 High-Performance Concrete for Marine Structures in Coastal Central Vietnam.Materials (Basel, Switzerland) · 2026
- Development of Alkali-Activated Phosphogypsum Mortar Incorporating Silica Fume and Metakaolin for Enhanced Durability and CO 2 MineralisationIOP Conference Series: Earth and Environmental Science · 2026
- Fracture behavior of carbon fiber reinforced coral aggregate seawater concreteEngineering Fracture Mechanics · 2025