Experimental Investigation and Taguchi Optimization of Print Parameters Affecting the Tensile Strength of 3D-Printed PLA Parts
Mehdi Moayyedian, Mohsen Hedayati-Dezfooli, Mohamed Fayed, Askhat Mussin, Vuk Cvorovic, Ibrahim Elbadawy
Key points
From the paper's conclusion- Experimental confirmation testing using the identified optimal combination (0.20 mm layer thickness, 90% infill, 40 mm/s retraction speed, and 80 mm/s travel speed) yielded a peak ultimate tensile strength of 36.6 MPa, achieving a 12.3% improvement over the initial experimental maximum.
Abstract
This study systematically investigates and optimizes the influence of Fused Deposition Modeling (FDM) process parameters on the macroscopic tensile strength of polylactic acid (PLA) components. Addressing the need for predictable structural performance in 3D-printed parts, the novelty of this work lies in establishing a holistic, multi-stage optimization framework that maps the combined kinematic and geometric interactions of critical printing parameters directly to structural failure mechanisms and microstructural integrity. A systematic four-phase methodology was executed using a Taguchi L25 orthogonal experimental design to evaluate four manufacturing variables, namely layer thickness (P1), infill percentage (P2), nozzle retraction speed (P3), and nozzle travel speed (P4) across five discrete levels. Uniaxial destructive tensile testing on an ST Series Universal Testing System revealed that the initial ultimate tensile strength spanned a broad range from 20.04 MPa to a peak of 32.59 MPa. Signal-to-noise (S/N) ratio analysis (“Larger-the-Better”) and Analysis of Variance (ANOVA) at a 95% confidence level established layer thickness (P1) as the strictly dominant governing factor (F = 5.56), contributing 43.14% to total system variance. Parametric impact tracking confirmed secondary physical contributions from retraction speed (P3, 20.86%) and infill percentage (P2, 16.82%), while nozzle travel speed (P4, 3.90%) exhibited a negligible effect. Experimental confirmation testing using the identified optimal combination (0.20 mm layer thickness, 90% infill, 40 mm/s retraction speed, and 80 mm/s travel speed) yielded a peak ultimate tensile strength of 36.6 MPa, achieving a 12.3% improvement over the initial experimental maximum. Ultimately, this research offers a highly predictable, mathematically validated manufacturing strategy for converting empirical FDM adjustments into reliable and solid engineering components.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Optimization of 3D Printing Parameters for Compressive Strength of PLA Using the Taguchi MethodThe Eurasia Proceedings of Science Technology Engineering and Mathematics · 2026
- Prediction of tensile strength of PLA parts produced with FDM using Taguchi L27, ANOVA, and large-scale machine learning models and optimal parameter designJournal of Thermoplastic Composite Materials · 2026
- Multi-Objective Optimization of the Mechanical Properties of 3D-Printed PLA: An Integrated Taguchi and NSGA-II Approach.Polymers · 2026
- Multi‐Response Optimization of FDM Process Parameters for PLA : The Strength–Energy–Roughness Trade‐Off via Taguchi, ANOVA , and Machine LearningJournal of Polymer Science · 2026
- Optimization of Flexural Strength of PLA Flexural Test Specimens Produced by FDM Using Taguchi L27 Orthogonal Array and Hybrid Regression ModelJournal of Polymer Science · 2026
- Effects of Printing Parameters on the Tensile Performance and Prediction of PLA-Based 3D Printed ObjectsMaterials Research Express · 2026