Journal of Composites Science

Matrix Densification Meets Crack Control: Steel Fiber-Reinforced High-Performance Concrete and Slag-Modified Mortar Under Sulfate Attack

Chahrazed Benkhedda, Abdelmadjid Berga, Tayeb Rikioui, Nazihe Terfaya, Zouaoui R. Harrat, Mohammed Chatbi, Fouad Boukhelf, Mohammed Benzerara,

Key points

From the paper's conclusion
  • Combining a dense, low water-to-binder matrix with steel-fiber crack control therefore appears promising for limiting early-age strength loss under sulfate exposure.

Abstract

Sulfate attack causes premature deterioration of reinforced concrete in arid and semi-arid regions through the formation of expansive gypsum and ettringite. This study combines local mineral additions and steel fibers to improve the strength and sulfate durability of materials made with regional resources from Béchar, Algeria. Three concretes were tested: ordinary concrete (BO), high-performance concrete (HPC), and steel-fiber-reinforced HPC (SFHPC), which contains silica fume at 8.1% of the cement mass (34 kg/m3) and 40 kg/m3 of corrugated steel fibers, together with a mortar in which 25% of the cement was replaced by ground industrial slag. The concretes were tested in compression and splitting tension after 28 days in potable water or 10% sodium sulfate solution; the mortar was tested in compression and flexure at 14 and 28 days and after two years of burial in sulfate soil. Sulfate curing lowered compressive strength by 9.32% (BO), 20.76% (HPC), and 10.97% (SFHPC), and splitting tensile strength by 19.81%, 18.19%, and 11.30%, respectively. SFHPC thus lost about half as much compressive strength as HPC and the least tensile strength, although its relative compressive loss slightly exceeded that of BO, whose absolute strength was about three times lower. Visually, SFHPC specimens remained held together by fibers after cracking, while BO failed by brittle spalling. After two years in soil containing 35% sodium sulfate, the mortar had a compressive strength 0.87% above and a flexural strength 14.78% below its 28-day values. Without same-age sulfate-free controls, these changes combine continued hydration and sulfate effects and do not directly measure sulfate resistance. Combining a dense, low water-to-binder matrix with steel-fiber crack control therefore appears promising for limiting early-age strength loss under sulfate exposure. Because the mixtures differ in several parameters, the separate effects of silica fume, water-to-binder ratio, and fibers could not be isolated, and longer exposure is needed to confirm long-term resistance. The approach also uses local and by-product materials for durable, low-clinker infrastructure.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Matrix Densification Meets Crack Control: Steel Fiber-Reinforced High-Performance Concrete and Slag-Modified Mortar Under Sulfate Attack — Science Skim