Wear Degradation of High-Nitrogen Austenitic Steels for Internal Combustion Engines in Hydrogen-Containing Alternative Fuels
Alexander I. Balitskii, Valerii O. Kolesnikov, Jarosław Chmiel, Valentina O. Balitska, Marcin A. Królikowski, Ljubomyr M. Ivaskevych
Key points
From the paper's conclusion- This study investigates hydrogen-assisted degradation of two cold-worked high-nitrogen Cr–Mn–N austenitic steels, DDT68 and P900, under dry rolling–sliding contact after controlled electrochemical hydrogen charging.
Abstract
The development of hydrogen and hydrogen-containing fuel infrastructure requires structural materials resistant to the combined effects of hydrogen exposure, cyclic contact stresses, and tribological loading. This study investigates hydrogen-assisted degradation of two cold-worked high-nitrogen Cr–Mn–N austenitic steels, DDT68 and P900, under dry rolling–sliding contact after controlled electrochemical hydrogen charging. Hydrogen uptake, wear intensity, microstructure, subsurface damage, and rolling contact fatigue (RCF) were analyzed comparatively. The mean grain size was approximately 25 μm for DDT68 and 43 μm for P900, while hydrogen concentrations were 15–17 and 12–14 ppm, respectively. Hydrogen increased the wear intensity of both steels, with wear acceleration factors ranging from approximately 2.1 to 10.0 for DDT68 and 1.4 to 4.2 for P900 over 200–600 N. The differences in wear intensity between DDT68 and P900 after hydrogen charging were statistically significant over the investigated load range. The finer-grained DDT68 exhibited greater hydrogen retention and a stronger hydrogen-associated wear response. The observed damage is consistent with HELP-assisted deformation localization, with possible contributions from HEDE and hydrogen–defect interactions, promoting subsurface microcracking, delamination, and spalling. Hertzian analysis located the maximum subsurface shear stresses approximately 0.035–0.062 mm below the contact surface. Finally, an indicator-based framework combining wear response, hydrogen content, and prescribed mass-loss reference levels is proposed for comparative durability assessment under the investigated conditions, rather than as a universally calibrated service-life prediction model.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Hollow specimen method for tensile tests in high-pressure hydrogen gas: The role of strain rate and surface qualityMRS Bulletin · 2026
- Mechanical properties of SS310 and IN625 following high-temperature hydrogen exposureFrontiers in Energy Research · 2026
- Burst tests of cold drawn and heat treated austenitic stainless steel (316L) tubes charged in pressurized hydrogenWelding in the World · 2026
- Fretting Wear of a 304L stainless steel in 200-bar pressurized hydrogen: A typical nodular third body structureWear · 2025
- Compatibility of cold drawn and heat treated austenitic stainless steel (316L) tube for green hydrogen applicationsWelding in the World · 2026
- Atomistic Insights into Hydrogen Diffusion and Deformation Mechanisms in FeCrNi-Based Austenitic Stainless Steels: Effects of Alloying, Temperature, and Hydrogen ConcentrationMolecules · 2026