Burst tests of cold drawn and heat treated austenitic stainless steel (316L) tubes charged in pressurized hydrogen
Sam Shaanika, Thomas Böllinghaus, Oded Sobol, Thomas S Alweendo, Eike Krafft, Satish Ravi
Federal Institute For Materials Research and Testing · University of Namibia
Key points
From the paper's conclusion- This study evaluates the strength and fracture behavior of both cold-drawn and heat-treated 316L austenitic stainless-steel tubular specimens fabricated from 1/2″ (12.7 mm) and 3/8″ (9.53 mm) tube after gaseous high-pressure pre-charging with wall thickness 0.5 mm.
Abstract
Abstract Global decarbonization targets are driving expansion of green hydrogen infrastructure, yet high-pressure hydrogen exposure can degrade the mechanical performance of critical stainless-steel components, typically made of the common steel 316L. This study evaluates the strength and fracture behavior of both cold-drawn and heat-treated 316L austenitic stainless-steel tubular specimens fabricated from 1/2″ (12.7 mm) and 3/8″ (9.53 mm) tube after gaseous high-pressure pre-charging with wall thickness 0.5 mm. Hydrogen concentration in the range between 76 and 100 ppm was measured in precharged sample in both states and the recorded quantity of 2–5 ppm in the non-precharged specimen. Hydrostatic burst tests at ambient temperature were carried out with precharged specimens and revealed an increase in burst pressure for both material states, as compared to non-precharged specimens as a reference. In addition, fractographic analysis by scanning electron microscopy has identified deeper dimples and wider microvoids in hydrogen-precharged specimens, indicating also some softening of the material in the cold-drawn as well as in the heat-treated state. As the time to failure also increased, it is anticipated that the hydrogen introduced in the specimens caused a respective increase in both, ductility in terms of the straining and deformation capacity, as well as an increase in strength. For engineering applications, the findings indicate some beneficial effect that, despite exposure to extreme hydrogen conditions, 316L tubes retain, and even modestly enhance, their structural integrity, supporting a safe deployment in green hydrogen transport and storage systems, at least at ambient temperature.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Compatibility of cold drawn and heat treated austenitic stainless steel (316L) tube for green hydrogen applicationsWelding in the World · 2026
- Hollow specimen method for tensile tests in high-pressure hydrogen gas: The role of strain rate and surface qualityMRS Bulletin · 2026
- Wear Degradation of High-Nitrogen Austenitic Steels for Internal Combustion Engines in Hydrogen-Containing Alternative FuelsEnergies · 2026
- Study on Hydrogen Embrittlement Behavior of 316L Austenitic Stainless Steel Based on Digital Image CorrelationJournal of Engineering Materials and Technology · 2026
- Mechanical properties of SS310 and IN625 following high-temperature hydrogen exposureFrontiers in Energy Research · 2026
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part I: Structure, Mechanical Properties and Susceptibility to Hydrogen EmbrittlementMetals · 2026