Key points
From the paper's conclusion- The findings suggest that reinforcement depends primarily on particle dispersion and interfacial stress transfer rather than chemical modification of the PMMA backbone.
Abstract
Background/Objectives: Auto-polymerized polymethyl methacrylate (PMMA) is widely used in denture repair, relining, and base-plate fabrication but is susceptible to fracture due to limited flexural strength and fatigue resistance. This in vitro study investigated the concentration-dependent effects of synthetic aluminosilicate clay (ASC) nanoparticles on the flexural strength, Vickers hardness, surface roughness, and microstructure of auto-polymerized PMMA. Methods: A total of 120 specimens of SR Triplex Cold were prepared with 0 (control), 1, 3, or 5 wt.% ASC (50-100 nm; n = 30/group). ASC was dispersed in the monomer by probe sonication for 10 min. After pressure curing and storage in distilled water at 37 °C for 7 days, flexural strength, Vickers hardness, and surface roughness (Ra) were measured (n = 10/test/group). Microstructural characterization employed SEM, EDX, and XRD. Data were analyzed using ANOVA with appropriate post hoc tests (α = 0.05). Results: ASC concentration significantly affected all three properties (p < 0.001). At 1 wt.% ASC, flexural strength increased from 61.50 ± 3.37 to 79.70 ± 2.11 MPa (+29.6%), and hardness increased from 84.39 ± 3.81 to 97.84 ± 2.56 VHN. At 3 and 5 wt.%, these properties declined to 52.60 ± 3.75 and 31.70 ± 2.83 MPa, and to 63.97 ± 2.94 and 27.73 ± 2.62 VHN, respectively. Surface roughness increased with ASC concentration, from 0.102 ± 0.012 µm (control) to 0.195 ± 0.013, 0.245 ± 0.022, and 0.327 ± 0.035 µm at 1, 3, and 5 wt.%, respectively. SEM revealed favorable particle dispersion, crack deflection, and particle bridging at 1 wt.%, whereas higher concentrations promoted agglomeration, microvoid formation, and interfacial debonding. XRD confirmed the coexistence of the amorphous PMMA phase and crystalline aluminosilicate reflections. Conclusions: Under the conditions tested, 1 wt.% ASC provided the most favorable balance of mechanical and surface properties, improving flexural strength and hardness while maintaining Ra below 0.2 µm. Higher concentrations compromised mechanical performance, with the 3 and 5 wt.% groups falling below the minimum flexural strength for Type 2 polymers. The findings suggest that reinforcement depends primarily on particle dispersion and interfacial stress transfer rather than chemical modification of the PMMA backbone.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Silver Nanoparticle Incorporation on the Flexural Strength and Color Stability of Heat-Polymerized Polymethyl Methacrylate (PMMA) Denture Base Resin: An In Vitro Study.Cureus · 2026
- Evaluation of mechanical and physical properties of PMMA-based acrylic composites containing nanoparticles for temporary filling materials.Proceedings of the Institution of Mechanical Engineers. Part H, Journal of engineering in medicine · 2026
- Effect of magnesium oxide nanoparticles on the flexural strength, surface roughness, and color of self-cure PMMA provisional crownsScientific Reports · 2026
- Comparative Analysis of the Mechanical and Biofilm Surface Formation of 3D Printed Resins and Milled PMMA Blocks With and Without Inorganic Fillers.Clinical and experimental dental research · 2026
- Comparative Evaluation of Flexural and Impact Strengths of Glass Fiber- and Titanium Dioxide Nanoparticle-Reinforced Polymethyl Methacrylate Denture Base Resin: An In Vitro Study.Cureus · 2026
- Production of Green Synthesized Zinc Oxide Nanoparticle-Reinforced PMMA-Based Photopolymer Resins on DLP-Based 3D Printers and CharacterizationPolymers · 2026