Proceedings of the Institution of Mechanical Engineers. Part H, Journal of engineering in medicine

Evaluation of mechanical and physical properties of PMMA-based acrylic composites containing nanoparticles for temporary filling materials.

Ahmed H Oleiwi, Saja A Moosa, Hussein K Dalfi

College of Engineering, Wasit University, Iraq. · College of Materials Engineering, University of Technology-Iraq, Baghdad, Iraq.

Key points

From the paper's conclusion
  • This study aims to investigate the effect of titanium dioxide (TiO2) nanoparticles on the mechanical and physical properties of polymethyl methacrylate (PMMA)-based acrylic composite materials suitable for temporary dental applications.

Abstract

This study aims to investigate the effect of titanium dioxide (TiO2) nanoparticles on the mechanical and physical properties of polymethyl methacrylate (PMMA)-based acrylic composite materials suitable for temporary dental applications. The samples were prepared using Orthocryl resin with 0, 1, 3, 5, 7, and 10 wt.% TiO2 added via a mold pressing technique. Tensile strength, elongation, elastic modulus, toughness, fracture toughness, hardness, wear resistance, density, water absorption, FESEM analysis, and FTIR analysis were investigated. Results showed that the enhancement in mechanical properties due to the increase of TiO2 concentration up to 7 wt.% is noticeable. The tensile strength rises from around 17 MPa for pristine material to about 41 MPa for 7 wt. % TiO2, elongation increases from around 1.3% to 3.5%. Elastic modulus increases from around 1.1 GPa-2.1 GPa for 10 wt. % TiO2, hardness increased from around 55 to 73 Shore D. Toughness increased from around 3.7 to 7.1 J/m2 for 7 wt.% TiO2, and fracture toughness increased from around 0.06 to 0.14 MPa·m1/2 for 10 wt.%. Furthermore, wear rate reduced with an increase in TiO2 concentration in the 5-7 wt.% range, but density rose from 1.10 to 1.165 g/cm3 and water absorption from 3.3% to 4.9%. FESEM analysis showed denser and more uniform microstructure of samples in case of moderate TiO2 concentration, whereas FTIR spectrum did not reveal any changes in chemical structure of acrylic resin matrix. In general, 7 wt.% TiO2 proved to be optimal for mechanical and tribological characteristics.